Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
Oxford Polymers PC 912 Unfilled Polycarbonate for Injection and Extrusion Molding Unfilled Polycarbonate for Injection and Extrusion MoldingInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
Polymer Resources PC-BR1-UV Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilized Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilizedFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical.. |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
Polymer Resources PC-FD3-[color]-1 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
Polymer Resources PC-GP1-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Low Flow Polycarbonate, FDA-compliant Feedstocks, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro.. |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
Polymer Resources PC-GP4-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Easy Flow Polycarbonate, FDA-compliant Feedstocks, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
Polymer Resources PC-GP4-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
Polymer Resources PPX-GP5 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 270F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Tensile Strength, Yield | 62.1 MPa @Thickness 3.17 mm |
9010 psi @Thickness 0.125 in |
ASTM D638 |
PTS Tristar® PC-10R-(18) 18 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 62.1 MPa @Thickness 3.17 mm |
9010 psi @Thickness 0.125 in |
ASTM D638 |
PTS Tristar® PC-10R-CL(V15) 15 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
Polymer Resources NY66-IM1 Nylon 66, Medium Impact Modified Nylon 66, Medium Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are te.. |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
Polymer Resources PC-FD2 Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
Polymer Resources PC-FD4 Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
Polymer Resources PC-GP3-D-[color]-1 Polycarbonate, General Purpose, High Flow with Mold Release Polycarbonate, General Purpose, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
Polymer Resources PC-UV4-[color]-1 Polycarbonate, UV-stabilized, Easy Flow with Mold Release Polycarbonate, UV-stabilized, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Tensile Strength, Yield | 62.1 MPa @Thickness 3.17 mm |
9010 psi @Thickness 0.125 in |
ASTM D638 |
PTS Tristar® PC-08 8 MFI Extrusion Grade Polycarbonate Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 62.1 MPa @Thickness 3.17 mm |
9010 psi @Thickness 0.125 in |
ASTM D638 |
PTS Tristar® PC-10FR-(16) 16 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
Fiberfil® J-69/10/E High performance polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
Fiberfil® J-69/10/E/UV High performance polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® PC200 Polycarbonate 20 melt superior processing, fast cyclingAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
Techmer ES Luriblend® PA6 TS15 BK Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Silicone Lubricant and PTFE LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composite.. |
|||
Tensile Strength, Yield | 62.1 MPa | 9010 psi | ASTM Data |
Styron CALIBRE™ 200 6 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Tensile Strength, Yield | 62.1 MPa | 9010 psi | ASTM Data |
Styron CALIBRE™ 2071 15 Polycarbonate, Sterilization Grade CALIBRE® 2071 resins are designed for those applications which use steam or ethylene oxide for sterilization while providing enhanced mold release characteristics. This material has excellent ret.. |
|||
Tensile Strength, Yield | 62.1 MPa | 9010 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 2091-15 Polycarbonate Resin Overview: CALIBREâ„¢ MEGARADâ„¢ 2091 Polycarbonate Resins are designed for single use medical devices (SUDs) that require gamma and electron-beam irradiation and an accelerated schedule for de.. |
|||
Tensile Strength, Yield | 62.1 MPa @Thickness 3.17 mm |
9010 psi @Thickness 0.125 in |
|
Samyang Trirex® PC-3022IR 15 MFI Clear Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 62.1 MPa | 9010 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate Resin Overview: CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate resin provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to hi.. |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
Techmer ES HiFill® PPSU A1 0200 B LE Availability: North AmericaForms: PelletsFeatures: High Density and Low ExtractablesAppearance: OpaqueInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | ISO 527 |
A. Schulman SCHULAMID® 6 GB30 30% Glass Bead Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
Ensinger Hydex™ 202 Rigid Polyurethane (PU) Hydex™ 202 is a totally rigid polyurethane resin that exhibits a broad range of chemical resistance, as well as superior impact and excellent mechanical properties. It can be used for any mechanic.. |
|||
Tensile Strength, Yield | 62.1 MPa | 9000 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® FRPC400 Polycarbonate, Flame-Retarded Flame-retarded V0, high impact injection molding polycarbonateAll information provided by LTL Color Compounders, Inc. |