Mechanical Properties Metric English Comments
Tensile Strength, Yield 59.8 MPa

@Thickness 3.20 mm
8680 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical Lupox® TE5000H PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provided by LG Chemical
Tensile Strength, Yield 59.8 MPa

@Thickness 3.20 mm
8680 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical Lupox® TE5000HU PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 26062-94-2, 137050-02-03 and 103598-77-2Information provided by LG Chemical
Tensile Strength, Yield 59.8 MPa

@Thickness 3.20 mm
8680 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical Lupox® TE5000HZ PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Door Handle)CAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provided by LG Chemical
Tensile Strength, Yield 59.8 MPa

@Thickness 3.20 mm
8680 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOY GN1008RF PC, Halogen Free, Flame Retardant, High impact strength
Description: Injection Molding, PC, Halogen Free Flame Retardant, High impact strengthApplication: IT&OA (Notebook PC battery pack housing)CAS: 103598-77-2, 137050-02-03 and 139189-30-3Information p..
Tensile Strength, Yield 59.8 MPa

@Thickness 3.20 mm
8680 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOY HG5000B PC/ABS, Heat Resistance
Description: Injection Molding, PC/ABS, High Gloss, Heat Resistance, High FlowApplication: E&E (housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Tensile Strength, Yield 59.8 MPa
8680 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® HR-1008B PC/ABS, Unreinforced
PC/ABS material that can be used for hand phone and car phoneInformation provided by Samsung Cheil Industries.
Tensile Strength, Yield 59.8 MPa
8680 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® NE-1050 PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 59.8 MPa
8680 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® NH-1027HF PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 59.8 MPa
8680 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® HR-1008B PC/ABS, Unreinforced
PC/ABS material that can be used for hand phone and car phoneInformation provided by Samsung Cheil Industries.
Tensile Strength, Yield 59.8 MPa
8680 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® NE-1050 PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 59.8 MPa
8680 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® NH-1027HF PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 59.8 MPa
8680 psi
ASTM D638
Cheng Yu Plastic FV3010 Polyformaldehyde
Tensile Strength, Yield 59.8 MPa
8680 psi
ASTM D638
Cheng Yu Plastic FV3015 Polyformaldehyde
Tensile Strength, Yield 59.8 MPa
8680 psi
ASTM D638
Cheng Yu Plastic FV3020 Polyformaldehyde
Tensile Strength, Yield 59.8 MPa
8680 psi
ASTM D638
Cheng Yu Plastic FV3025 Polyformaldehyde
Tensile Strength, Yield 59.8 MPa
8680 psi
ASTM D638
Cheng Yu Plastic FV3030 Polyformaldehyde
Tensile Strength, Yield 59.8 MPa
8680 psi
ASTM D638
Cheng Yu Plastic FV3035 Polyformaldehyde
Tensile Strength, Yield 59.8 MPa
8680 psi
ASTM D638
Cheng Yu Plastic FV3050 Polyformaldehyde