Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 57.2 MPa | 8300 psi | ASTM D638 |
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Tensile Strength, Yield | 57.2 MPa | 8300 psi | ASTM D638 |
Polymer Resources TP-FR2-[color]-WR Polybutylene Terephthalate, Flame Retardant, Wear Resistant Polybutylene Terephthalate, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Tensile Strength, Yield | 57.2 MPa | 8300 psi | ASTM D638 |
Ravago Manufacturing Americas Hybrid S464 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 57.2 MPa | 8300 psi | ASTM D638 |
PTS Trimid® N66-T100HL Toughened, Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 57.2 MPa | 8300 psi | ASTM D638 |
Ravago Manufacturing Americas Hybrid B2035I Polycarbonate + PBT Alloy Available in North America High Impact Resistance Form: PelletsInformation provided by Ravago |
|||
Tensile Strength, Yield | 57.2 MPa | 8300 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® PAHF Polycarbonate-ABS Alloy General purpose HB-rated PC/ABS with improved chemical resistanceAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 57.2 MPa | 8300 psi | ASTM D638 |
Star Plastics PC/PET7901 Molding Grade PC/PET Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 57.2 MPa | 8300 psi | ASTM D638 |
Star Plastics PC20NBR Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 57.2 MPa | 8300 psi | ASTM D638 |
Techmer ES HiFill® PC R GY143 Availability: North AmericaForms: PelletsFeatures: Low Smoke EmissionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 57.2 MPa | 8300 psi | ASTM D638 |
Clariant Renol BR7039 Nylon 6 Alloy, bondable to TPU Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 57.2 - 61.4 MPa | 8300 - 8900 psi | ASTM D638 |
Alcoa KAMA 4223 Impact Modified RPET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 50”Silicone coatingCl.. |
|||
Tensile Strength, Yield | 57.2 - 85.0 MPa | 8300 - 12300 psi | Average value: 68.7 MPa Grade Count:4 |
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max.. |