Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EM3110 PC (Asia Pacific) Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Asia Pacific) Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer (Asia Pacific) Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f.. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer (Asia Pacific) Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXL1484T PC Copolymer Lexan* EXL1484T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in c.. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and up to 25% post consumer recycle content. Availability of resin is restricted and lead times are.. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXE1414 PC Copolymer Lexan* FXE1414 polycarbonate (PC) siloxane copolymer resin is a special effects fluorescent, medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductil.. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | ISO 527 |
SABIC Innovative Plastics LNP FARADEX DS0036I PC LNP* FARADEX* DS0036I is a compound based on Polycarbonate resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, No.. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DI001E PC (Europe-Africa-Middle East) LNP* Lubricomp* DI001E is a compound based on Polycarbonate resin containing Silicone. Added features include: Internally Lubricated, Easy Molding. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | |
Covestro Makroblend® UT-408 Polycarbonate + Polyester Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015,.. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | ISO 527-1 |
Kareline Oy PPMS5050 Natural Fiber Reinforced Polypropylene for injection molding Natural fiber reinforced thermoplastic composite for injection molding. Fiber ECF bleached softwood pulp. Matrix plastic polypropylen.Information provided by Kareline Oy Ltd |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Stat-kon DX92440 PC LNP STAT-KON* DX92440 is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive.This data was supplied.. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Asia Pacific) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | ISO 527-2 |
Styron Pulse® 2000EZ PC/ABS Engineering ResinInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | SABIC - Japan Method |
SABIC Innovative Plastics NORYL LEN2211 PPE+HIPS (Asia Pacific) PPE / HIPS unfilled, FR for LED application |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL 731 PPE+PS PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi.. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | ISO 527-1/-2 |
Covestro Bayblend® KU 2-1514 BBS073* Polycarbonate + ABS, Flame Retardant Grade Developmental productHigh heat resistant injection molding gradeimproved chemical resistance and stress cracking behavior compared to KU 2-1514ball indentation temperature = 125 °CVicat/B 120 tempe.. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® S600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 NC010 is an unreinforced lubricated medium high viscosity polybutylene terephthal.. |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
Chi Mei Wonderloy® PC-510 PC/ABS Alloy - Flame Retardant High Flow |
|||
Tensile Strength, Yield | 57.0 MPa | 8270 psi | 50mm/min; ISO 527 |
BASF Ultradur B 4520 BK00110 PBT Ultradur B 4520 BK00110 is a medium viscosity, pigmented black, rapidly freezing injection molding grade. |
|||
Tensile Strength, Yield | 57.0 MPa @Temperature 23.0 °C |
8270 psi @Temperature 73.4 °F |
5mm/min (0.2in/min); ASTM D638 |
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con.. |