Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 450 MPa | >= 65300 psi | |
MetalTek MTEK 410 Cast UNS J91150 Martensitic Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 450 MPa | >= 65300 psi | |
MetalTek MTEK SD100 Cast UNS J93380 Duplex Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Yield | 450 MPa @Strain 0.200 %, Temperature 871 °C |
65300 psi @Strain 0.200 %, Temperature 1600 °F |
|
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F) Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Tensile Strength, Yield | 450 - 620 MPa | 65300 - 89900 psi | |
Materion Brush 1915™ Heat Treated Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |
|||
Tensile Strength, Yield | >= 450 MPa | >= 65300 psi | |
MetalTek FERRALIUM® 225 UNS J32550 Duplex Stainless Steel Excellent seawater corrosion resistance combined with nearly twice the strength of common stainless steels. Produced under license of Meighs Ltd.Applications: Offshore piping systems, couplings. Cen.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 0.200 % |
65300 psi @Strain 0.200 % |
|
Haynes 242® alloy, cold reduced sheet, annealed Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 0.200 %, Temperature 760 °C |
65300 psi @Strain 0.200 %, Temperature 1400 °F |
|
Haynes 242® alloy, cold rolled sheet, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 0.200 % |
65300 psi @Strain 0.200 % |
Solution Annealed. Value at room temperature |
Special Metals INCONEL® Alloy 601 A nickel-chromium alloy with an addition of aluminum for outstanding resistance to oxidation and other forms of high-temperature corrosion. It also has high mechanical properties at elevated temper.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 0.200 %, Temperature 650 °C |
65300 psi @Strain 0.200 %, Temperature 1200 °F |
Precipitation Hardened prior to test |
Special Metals NIMONIC® Alloy 263 A precipitation-hardenable nickel-chromium-cobalt alloy with an addition of molybdenum for solid-solution strengthening. It has high strength and corrosion resistance along with good formability an.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 0.200 % |
65300 psi @Strain 0.200 % |
Precipitation Hardened. Value at room temperature |
Special Metals NIMONIC® Alloy PE16 A precipitation-hardenable nickel-iron-chromium alloy with an addition of molybdenum for solid-solution strengthening. It has good strength and oxidation resistance at temperatures to about 1380°.. |
|||
Tensile Strength, Yield | >= 450 MPa | >= 65300 psi | After bake hardening |
SSAB Tunnplat Docol® 600DL High-strength Steel High-strength SteelComments: Docol DP - Cold Rolled Steel - Extra high-strength steel (EHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm. Iron content is approximate - exact.. |
|||
Tensile Strength, Yield | >= 450 MPa @Strain 0.200 % |
>= 65300 psi @Strain 0.200 % |
|
Schmolz + Bickenbach UGICHROM 4462 Duplex Chrome Plated Bar Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 0.200 % |
65300 psi @Strain 0.200 % |
Typical |
TIMET CP Titanium (ASTM Grade 3) Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4900. Germany Aerospace: 3.7055. France: T-50. UK Aerospace Specification DTD 5023, 5273.Features: The mechanical properti.. |
|||
Tensile Strength, Yield | 450 MPa | 65300 psi | 0° |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass Balanced fabric 300 g/m2 Information provided by HexCel |
|||
Tensile Strength, Yield | >= 450 MPa @Strain 0.200 % |
>= 65300 psi @Strain 0.200 % |
|
CLAL-MSX CUPROROR® TL5 Spring, Copper Alloy Alloy especially suited to applications in electronics and electro technology. This doped copper, displays high electrical and thermal conductivity, good mechanical properties and excellent temperat.. |
|||
Tensile Strength, Yield | >= 450 MPa @Strain 0.200 % |
>= 65300 psi @Strain 0.200 % |
|
CLAL-MSX NICLAL 3444 H14 4/4 Hard Copper Alloy, diameter < 8 Copper Alloy, Free Cutting Bronze Main Characteristics: Excellent machineabilityHigh mechanical propertiesSelf lubricating alloyTypical Applications:Parts for connectorsFriction partsBearings-Pinions-Lock pinsInformation provided b.. |
|||
Tensile Strength, Yield | >= 450 MPa @Strain 0.200 % |
>= 65300 psi @Strain 0.200 % |
|
CLAL-MSX ARCAP Anticorrosion AP4 H12 1/2 hard, Rolled Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 0.200 % |
65300 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Grade 3 Titanium (UNS R50550) Uses: CPI equipment, industrial components, heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Tensile Strength, Yield | >= 450 MPa | >= 65300 psi | |
ArcelorMittal Dual Phase 780 Very high strength steel, Hot Rolled Steel Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martensitic or bainitic phase is dispersed in a soft .. |
|||
Tensile Strength, Yield | 450 - 550 MPa | 65300 - 79800 psi | |
ArcelorMittal Dual Phase 780 Y450 Very high strength steel, Cold Rolled Steel Available in the following: HCT780X (uncoated), HCT780X+ZE (electrogalvanized) and HCT780X+Z/ZF (Extragal®/Galvannealed)Description: Dual Phase steels offer an outstanding combination of strength a.. |
|||
Tensile Strength, Yield | 450 MPa | 65300 psi | |
Resistalloy International Resistalloy 3718 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |
|||
Tensile Strength, Yield | 450 MPa | 65300 psi | |
Resistalloy International Resistalloy 6015 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 0.200 %, Temperature 705 °C |
65300 psi @Strain 0.200 %, Temperature 1300 °F |
|
Haynes 242® alloy, hot rolled plate, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 0.200 % |
65300 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Grade 12 Titanium (UNS R53400) Uses: heat exchangers, industrial components, tubing, CPI equipment.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Tensile Strength, Yield | >= 450 MPa | >= 65300 psi | Minimum Guaranteed |
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT650 Heat Treatment) Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The g.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 0.200 % |
65300 psi @Strain 0.200 % |
|
Haynes 230® alloy plate, 16000 hours exposure at 649°C (1200°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |