Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 43.2 MPa | 6270 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L7005 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon L7005 is recommended for whites and light pastel colors only.Note: Physical properties based on L7005 tan 3210 sample.Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.2 MPa | 6270 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L7007 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon L7007 is recommended for whites and light pastel colors only.Geon L7007 is a higher gloss version of L7005.Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.2 MPa @Thickness 3.20 mm |
6270 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUCEL FW715CS Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 471-34-1Information provided by LG .. |
|||
Tensile Strength, Yield | 43.2 MPa | 6260 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SBB 3616 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Ultra High Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation P.. |
|||
Tensile Strength, Yield | 43.2 MPa | 6270 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 3500 Description: Natural, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 43.2 MPa | 6270 psi | ASTM D412 |
C.O.I.M. LARIPUR® LPR7025 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Tensile Strength, Yield | 43.2 MPa | 6260 psi | ASTM D-638 |
Axiall 3101 Rigid PVC, Extrusion Georgia Gulf 3101 is a powder blend designed for the extrusion of window, door and fence profiles where weatherability is of primary consideration.Information provided by Georgia GulfGeorgia Gulf be.. |
|||
Tensile Strength, Yield | 43.2 MPa | 6260 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SBF 3758 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact AcceptableUses: Shrink Wrap Forms: Pellets Processing Method: Blown FilmInformation Provided by Teknor Apex |