Polymer Property : Tensile Strength, Yield = 414 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 414 MPa
60000 psi
Niagara LaSalle 1215 Cold Finished Steel Bar
The A.I.S.I. grade 1215 has essentially eliminated a number of similar free machining grades, such as 1212. Both 1215 and 1213 machine considerably faster than 1212 and provide good surface finish a..
Tensile Strength, Yield 414 MPa
60000 psi
Pacific Sintered Materials FX-232-T Infiltrated High Carbon Steel Powdered Metal
Good strength, shock resistance and hardenability. Moderate tolerance control.Equivalent MPIF Specification: FX-1008-50All information provided by Pacific Sintered Metals.
Tensile Strength, Yield 414 MPa
60000 psi
PSM Industries Pacific Sintered Metals Infiltrated High Carbon Steel FX-232-T Powdered Metal
Good strength, shock resistance and hardenability, Moderate tolerance control Equivalent MPIF Specification: FX-1008-50Information Provided by Pacific Sintered Metals, a division of PSM Industries
Tensile Strength, Yield 414 MPa

@Temperature 23.9 °C
60000 psi

@Temperature 75.0 °F
0° Direction, Dry; 325°F Autoclave Cured; ASTM D638
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 581 Quartz Reinforced
Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock..
Tensile Strength, Yield 414 MPa
60000 psi
Performance Alloys MoldStar® 21 (PAS 21) Bronze Mold Alloy
Description: MoldStar® 21 bronze alloy provides good bearing qualities and resistance to wear, abrasion, fatigue, deformation and corrosion.Applications: Lifter BladesSlidesGibsWear PlatesEjector S..
Tensile Strength, Yield 414 - 483 MPa

@Strain 0.200 %
60000 - 70000 psi

@Strain 0.200 %
Materion BrushCAST® 275CT Fine Grain Casting Alloy (As Cast & Aged)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Tensile Strength, Yield 414 - 517 MPa
60000 - 75000 psi
Meehanite Ductliron® SP-80 Nodular Graphite Ductile Iron
Type SP-80 possesses in the as-cast condition more than twice the strength of conventional gray cast iron in combination with exceptional toughness. It has a predominantly pearlitic structure, is r..
Tensile Strength, Yield 414 MPa

@Strain 0.200 %,
Temperature 260 °C
60000 psi

@Strain 0.200 %,
Temperature 500 °F
Haynes Hastelloy® C-22® alloy, all-weld metal, GMAW short arc
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Yield 414 MPa
60000 psi
HP Alloys Alloy 718, 0% Cold Worked, Not Aged
0% Cold Worked, Not Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes ..
Tensile Strength, Yield 414 MPa

@Strain 0.200 %
60000 psi

@Strain 0.200 %
Heat Treated
Universal Wire Works 29-9 (AMS 5784) Filler Metal
Universal 29-9 is designed for welding similar and dissimilar corrosion and heat resisting steels with the gas metal arc and gas tungsten arc welding processes.Information provided by Universal Wire..
Tensile Strength, Yield 414 MPa

@Strain 0.200 %
60000 psi

@Strain 0.200 %
Universal Wire Works 316 Stainless Steel (AMS 5692) Filler Metal
Universal 316 is a chromium-nickel alloy with large amounts of molybdenum added for superior corrosion resistance and strength. The corrosion resistance is superior to types 302 and 304 making 316 t..
Tensile Strength, Yield >= 414 MPa
>= 60000 psi
ThyssenKrupp 12Ni5 Structural Steel
5% nickel steel for low temperature service down to -165°FApplication for pressure vessels and tanks for the transportation and storage of ethyleneReference: 5.000 t/y in thicknesses up to 2 in.Hea..
Tensile Strength, Yield 414 MPa
60000 psi
AR-5% O2
Universal Wire Works ER90SB-9 Steel Welding Wire
Universal 90S-B9 is used primarily for welding the higher chromium alloyed 9CrMoNbV steels A213 (T-91), A335 (p-91), A387 (Gr-91) used where elevated temperatures and pressures are required. The adv..
Tensile Strength, Yield >= 414 MPa

@Strain 0.200 %
>= 60000 psi

@Strain 0.200 %
Universal Wire Works Inconel 625 (AMS 5837) Filler Metal
Inconel Filler Metal 625 is recommended for gas metal arc and gas tungsten arc welding of nickel base alloys 625 and 601, Incoloy alloys, carbon steels, low alloy steels and stainless steels. This a..
Tensile Strength, Yield 414 MPa

@Strain 0.200 %
60000 psi

@Strain 0.200 %
Universal Wire Works 347 Stainless Steel (AMS 5680) Filler Metal
Universal 347 is extensively used with the gas tungsten arc, gas metal arc and submerged arc processes. This alloy is suitable for welding stabilized steel grades 321, 347 and 348. Alloy 347 should ..
Tensile Strength, Yield >= 414 MPa
>= 60000 psi
0.2% offset
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Hard
19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect..
Tensile Strength, Yield 414 - 469 MPa
60000 - 68000 psi
0.2% offset
Eagle Brass 210 Gilding Metal, Extra Spring
CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi..
Tensile Strength, Yield 414 - 462 MPa
60000 - 67000 psi
0.2% offset
Eagle Brass 220 Commercial Bronze, Extra Hard
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
Tensile Strength, Yield 414 - 538 MPa
60000 - 78000 psi
0.2% Offset
Eagle Brass 430 Ferritic Stainless Steel, 1/4 Hardened
Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro..
Tensile Strength, Yield 414 - 607 MPa
60000 - 88000 psi
0.2% offset
Eagle Brass 762 Nickel Silver 12%, 1/2 Hard
762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s..
Tensile Strength, Yield 414 MPa

@Strain 0.200 %
60000 psi

@Strain 0.200 %
Crucible Steel 440A Chromium Steel
Crucible 440A is a hardenable chromium steel which is the toughest of the high chromium cutlery grades. This grade is magnetic at all times. Information provided by Crucible Specialty Metals.
Tensile Strength, Yield 414 MPa
60000 psi
Premium Forging (Hot Forged, Heat Treated, and Cold Worked to less than 1" thick)
CMW® 3 Copper Alloy
CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre..
Tensile Strength, Yield 414 MPa

@Strain 0.200 %
60000 psi

@Strain 0.200 %
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 0% Cold Reduction
Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good ..
Tensile Strength, Yield 414 MPa

@Strain 0.200 %
60000 psi

@Strain 0.200 %
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 0% Cold Reduction + Aged 538°C (1000°F)/4hr/AC
Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good ..
Tensile Strength, Yield 414 MPa

@Strain 0.200 %
60000 psi

@Strain 0.200 %
ATI Allvac® Nickelvac® L-605 Cobalt-Nickel Superalloy, Heat Treatment: 1204°C (2200°F) Anneal
Data provided by Allvac.Applications: High temperature applications, jet engine components, devices in high fatigue service.
Tensile Strength, Yield 414 MPa

@Strain 0.200 %
60000 psi

@Strain 0.200 %
Carpenter Gall-Tough® Stainless
Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1..
Tensile Strength, Yield 414 MPa
60000 psi
Offset not specified
Carpenter HyMu "80"® Electronic Alloy, Cold Drawn Bar
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Tensile Strength, Yield >= 414 MPa
>= 60000 psi
For flat products (<4" thickness) and seamless tube and pipe
ATI Allegheny Ludlum AL Altemp® 625 Nickel-Base Superalloy, UNS N06625
Allegheny Ludlum Altemp 625 alloy is an austenitic nickel-base superalloy possessing excellent resistance to oxidation and corrosion over a broad range of corrosive conditions, including jet engine ..
Tensile Strength, Yield 414 MPa
60000 psi
Solution Annealed
ATI Allegheny Ludlum Altemp® 263 Nickel-Based alloy
Characteristics: high strength up to 1500°F, oxidation resistance up to 2000°FInformation provided by Allegheny Ludlum
Tensile Strength, Yield 414 MPa

@Strain 0.200 %
60000 psi

@Strain 0.200 %
Special Metals INCOLOY® 27-7MO Super-Austenitic Stainless Steel
INCOLOY® alloy 27-7MO (UNS S31277; EP 1,263,999 B1) is an advanced 7% molybdenum super-austenitic stainless steel offering corrosion resistance in most environments superior to 6% molybdenum super-..