Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.83 MPa | 700 psi | at 100%; ASTM D412 |
5286 Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | @50% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 592 Perfluoroelastomer Chemraz® 592, a versatile perfluoroelastomer developed with a proprietary filler system, is very resistant to plasma attack. This compound’s durometer allows for some hardware finish incons.. |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | ASTM D638 |
Multibase Multi-Flex® G 7150 TPE Styrene Ethylene Butylene Styrene Block Copolymer Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInforma.. |
|||
Tensile Strength, Yield | 4.83 MPa @Strain 300 % |
700 psi @Strain 300 % |
ASTM D412 |
Multibase Multi-Flex® G 7155 TPE Styrene Ethylene Butylene Styrene Block Copolymer Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInforma.. |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 6221 CUV Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | Tensile strength decreases by 15% after dry heat aging for 70 hrs at 437°F.; ASTM D412 |
Saint-Gobain COHRlastic® 400 General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | Tensile strength decreases by 15% after dry heat aging for 70 hrs at 437°F.; ASTM D412 |
Saint-Gobain COHRlastic® 600 General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3310-70 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | 100%; ASTM D412 |
Teknor Apex Flexalloy® 3500-65 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te.. |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | 3; ASTM D412 |
Teknor Apex Flexalloy® 3501-35-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Tensile Strength, Yield | 4.83 MPa @Strain 300 % |
700 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1805 Thermoplastic Elastomer Notes: Semi-transparent Features: High FlowInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2740 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2820M Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2825E Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 4.83 MPa @Strain 300 % |
700 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 7002 Thermoplastic Elastomer Notes: Semi-transparent Features: Good Chemical and Oil ResistanceInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | Tensile strength decreases by 15% after dry heat aging for 70 hrs at 437°F.; ASTM D412 |
Saint-Gobain COHRlastic® 500 General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | Tensile strength decreases by 10% after dry heat aging for 70 hrs at 437°F.; ASTM D412 |
Saint-Gobain COHRlastic® 9060 Wide Series General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | ASTM D412 |
Saint-Gobain COHRlastic® EC102 RFI/EMI Shielding, Electrically-Conductive Silicone Description: EC102 electrically-conductive silicone performs three distinct functions: the cabon filler in it allows it to act as a low amperage conductor; it shields RF and EM interference; and it .. |
|||
Tensile Strength, Yield | 4.83 MPa @Strain 300 % |
700 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1527 Thermoplastic Elastomer Notes: Translucent Features: Good Flow; Tough; Good Melt StrengthInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex Monprene® MP-2820M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex Monprene® MP-2825E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex UNIPRENE® 7010-64 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® IT 38-113 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalUV StabilizedApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First Cho.. |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3840MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTransparentUV StabilizedApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Tensile Strength, Yield | 4.83 MPa @Strain 300 % |
700 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3870MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTranslucentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | at 100%; ASTM D412 |
EG85A Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-4050 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionIndustrialConsumer GoodsProcessing Method:ExtrusionPolyOne.. |
|||
Tensile Strength, Yield | 4.83 MPa @Strain 300 % |
700 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-4070 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionIndustrialConsumer GoodsProcessing Method:ExtrusionInforma.. |
|||
Tensile Strength, Yield | 4.83 MPa | 700 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® ST-6140 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalOver-Molding GradeApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne Firs.. |