Teknor Apex Monprene® MP 7002 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Teknor Apex Company
Trade Name MONPRENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Monprene® MP 7002 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Notes: Semi-transparent Features: Good Chemical and Oil ResistanceInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
ASTM D792
Melt Flow 13.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
13.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
ASTM D2240
Tensile Strength at Break 8.27 MPa
1200 psi
ASTM D412
Tensile Strength, Yield 4.83 MPa

@Strain 300 %
700 psi

@Strain 300 %
ASTM D412
Elongation at Break 650 %
650 %
ASTM D412