Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 37.2 MPa | 5400 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 30-005W Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Oxford Polymers INJ-FR Glass Fiber Reinforced ABS, Flame Retardant Glass Fiber Reinforced ABS, Flame RetardantInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2000STHL Nylon 6 (Cond) Information provided by Ravago. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2000STL Nylon 6 (Cond) Information provided by Ravago. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Ravago Manufacturing Americas Hysun™ 383 ASA
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | 2 in/min; ASTM D638 |
Ineos H44N-00 Polypropylene Homopolymer H44N-00 is a high flow rate, nucleated polypropylene homopolymer designed for compounding and injection molding applications. The grade benefits from a high stiffness and isotropic shrinkage to help.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Techmer ES Elastoblend® PBT E IM SL3 Availability: North AmericaForms: PelletsAdditive: Impact Modifier and Silicone LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Spartech SP-9020 Premium ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Techmer ES HiFill® TPX-PVDF-03009 C Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerFeatures: Low Shrinkage and Low Smoke EmissionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Techmer ES Plastiblend® ABS E Availability: North AmericaForms: PelletsFeatures: High ViscosityProcessing Method: Blow Molding and ExtrusionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM Data |
Styron Magnum™ 2630 ABS, High Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM Data |
Styron Magnum™ 8325 ABS, Sheet Coextrusion Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
PlastxWorld CEVIAN® E80 ABS Inherently Static Dissipative Transparent ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | |
Tra-Con Tra-Bond FS227 Thixotropic Epoxy/Polyamide Adhesive TRA-BOND FS227 is a thixotropic (thick paste) polymer epoxy/polyamide system developed for industrial adhesive and sealing applications where the combination of high fill, easy handling, good wettin.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Eastman Tenite 307E0V16310 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Eastman Tenite Butyrate 285A2R30016 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 8%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Eastman Tenite Propionate 380A4000010 Clear, Trsp Cellulose Acetate Propionate Plasticizer 10%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ASA T-105 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers NPP30-1200S Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers SBS 2160 Clear Styrene Butadiene Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Clariant Renol PP1112AS10 Polypropylene, Static Dissipative Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | 2 in/min (50 mm/min); ASTM D-638 |
Bapolene® 4052F Polypropylene, Blown Film Grade Bapolene PP4052F is a PP homopolymer for blown film applications. It contains slip and antiblock additives as processing aids. It offers good clarity and optical properties. This product meets FD.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | |
Atom Adhesives AA-BOND FS227 Epoxy Adhesive AA-BOND FS227 is a thixotropic polymer epoxy/polyamide system developed for industrial adhesive and sealing applications where the combination of high fill, easy handling, good wetting, toughness, a.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Aaron Industries AVPP HOMO 200-1 Virgin Polypropylene A virgin polypropylene specifically designed for all injection molding applications. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Amco Amalloy® B1044 Polymer Alloy Amco Amalloy B1044 is a proprietary copolymer with exceptional clarity and toughness.Low haze, low melt flow, high tensile & flexural strength.Information provided by Amco Plastic Materials. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Albis Plastics ASA 02A MR20 , 20% Mineral Filled
(discontinued **) Acrylonitrile/Styrene/AcrylateCharacteristics: Excellent UV, Good Rigidity, Good Dimensional StabilityApplications: Sunglasses, Boat Shells, Roofs for Campers & RVsProcessing: Injection Molding (Mel.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Eastman Tenite Propionate 350E0096914 Natural, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 25% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |