Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 331 MPa @Temperature 23.9 °C |
48000 psi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 7781 E-Glass Reinforced Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low .. |
|||
Tensile Strength, Yield | 331 MPa @Strain 0.200 %, Temperature 538 °C |
48000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Kennametal Stellite Stellite® 31 PM with P/M Processing; heat treated at 93°C (200°F) and water quenched Typical applications include, miscellaneous wear parts. Data provided by the manufacturer, Deloro Stellite Inc.Product of former Deloro Stellite Inc. |
|||
Tensile Strength, Yield | 331 MPa @Strain 0.200 %, Temperature 538 °C |
48000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Hastelloy® G-30® alloy, all-weld metal, GTAW weld 3.2 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 331 MPa @Strain 0.200 %, Temperature 538 °C |
48000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Ultimet® alloy, 19.1 mm thick plate, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 331 MPa @Strain 0.200 %, Temperature 316 °C |
48000 psi @Strain 0.200 %, Temperature 601 °F |
|
Haynes Ultimet® alloy, 6.3-38.1 mm plate Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 331 MPa @Strain 0.200 % |
48000 psi @Strain 0.200 % |
|
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet, GTAW weld HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 331 MPa @Strain 0.200 % |
48000 psi @Strain 0.200 % |
|
Special Metals INCOLOY® 25-6M0 Super Austenitic Stainless Steel (UNS N08926) Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Yield | >= 331 MPa | >= 48000 psi | |
Wingate Alloys Winco NT 24 Nitrogen-Strengthened Austenitic Stainless Steel Winco NT 24 provides good aqueous corrosion resistance combined with resistance to abrasives, metal-to-metal wear and sustained heats of 1500°F. Higher mechanical properties than standard austeniti.. |
|||
Tensile Strength, Yield | >= 331 MPa | >= 48000 psi | |
Alcoa Deltalloy® 4032-T651 Aluminum Weldability = B; Stress Corrosion Cracking Resistance = B; General Corrosion Resistance = C (A = best; E = worst). General 4032 characteristics and uses: Good machinability and drilling characterist.. |
|||
Tensile Strength, Yield | 331 - 393 MPa | 48000 - 57000 psi | 0.2% offset |
Eagle Brass 110 EPT COPPER, Spring Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Tensile Strength, Yield | 331 - 400 MPa | 48000 - 58000 psi | 0.2% offset |
Eagle Brass 240 Low Brass, 3/4 Hard CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib.. |
|||
Tensile Strength, Yield | 331 - 538 MPa | 48000 - 78000 psi | 0.2% offset |
Eagle Brass 752 Nickel Silver 18%, 1/2 Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Tensile Strength, Yield | 331 - 393 MPa | 48000 - 57000 psi | 0.2% offset |
Eagle Brass 101 OFE COPPER (Certified), Spring Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Strength, Yield | 331 - 393 MPa | 48000 - 57000 psi | 0.2% offset |
Eagle Brass 102 OF COPPER (Non-Certified), Spring Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Tensile Strength, Yield | 331 MPa @Strain 0.200 % |
48000 psi @Strain 0.200 % |
|
Carpenter 20Cb-3® Stainless Steel, Bar, Annealed at 1750°F (955°C) then Water Quenched Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Yield | 331 MPa | 48000 psi | In rolling direction |
AK Steel CARLITE® M-3 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |
|||
Tensile Strength, Yield | 331 MPa | 48000 psi | In rolling direction |
AK Steel CARLITE® M-4 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |
|||
Tensile Strength, Yield | 331 MPa | 48000 psi | In rolling direction |
AK Steel CARLITE® M-6 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |
|||
Tensile Strength, Yield | 331 MPa | 48000 psi | Semi-Processed |
AK Steel DI-MAX® M-47 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Tensile Strength, Yield | 331 MPa | 48000 psi | Typical |
ATI Allegheny Ludlum Type 441 Alloy Stainless Steel Allegheny Ludlum stainless Type 441 alloy is a heat resisting ferritic grades providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dual stab.. |
|||
Tensile Strength, Yield | >= 331 MPa @Strain 0.200 % |
>= 48000 psi @Strain 0.200 % |
|
Carlson Nitronic® 30® Austenitic Stainless Steel General DescriptionNitronic 30 is a nitrogen-strengthened austenitic stainless steel developed for applications requiring good aqueous corrosion resistance combined with good resistance to abrasive .. |
|||
Tensile Strength, Yield | 331 MPa | 48000 psi | In rolling direction |
AK Steel CARLITE® M-5 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |