Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 275 MPa @Strain 0.200 % |
39900 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4305 Austenitic Stainless Steel Good general corrosion resistance.Applications: Where machinability is required - threaded bar, studs, domestic appliances.Available in bar and rod forms. |
|||
Tensile Strength, Yield | 275 - 450 MPa @Strain 0.200 % |
39900 - 65300 psi @Strain 0.200 % |
|
Kobe Steel KS60 Commercially Pure Titanium, ASTM Gr. 2, Annealed Nominal Composition: Ti-Fe-OApplications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Relatively high strength, excellent corrosion resistance.. |
|||
Tensile Strength, Yield | 275 - 450 MPa | 39900 - 65300 psi | 0.2% proof |
Kobe Steel KS60AKOT Titanium alloy with low alloying elements, ASTM Gr. 33, Annealed Nominal Composition: Ti-0.4 Ni-0.015 Pd-0.025 Ru-0.14 Cr Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant... |
|||
Tensile Strength, Yield | 275 - 450 MPa | 39900 - 65300 psi | 0.2% proof |
Kobe Steel Titanium alloy with low alloying elements, ASTM Gr. 7, Annealed Nominal Composition: Ti-0.15 Pd Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant. Information provided by .. |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
MetalTek MTEK 230 Cast UNS C95500 Aluminum Bronze Versatile alloy with high strength, good ductility, unusual toughness, plus exceptional wear resistance. Aluminum Bronze heat treated to higher mechanical properties where necessary.Information prov.. |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
MetalTek MTEK 23-35WCo Heat Resistant Stainless Steel Information provided by MetalTekCast ASTM A297 MOD. |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
MetalTek MTEK N-12MV Cast UNS N30012 Severe Corrosion and Heat Resistant Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
MetalTek MTEK N-7M Cast UNS N30007 Severe Corrosion and Heat Resistant Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
MetalTek WCB UNS J13345 Cast Alloy Steel General structural use.Applications: Cylinders, rolls, hollow shafts.Information provided by MetalTek |
|||
Tensile Strength, Yield | 275 MPa @Temperature 870 °C |
39900 psi @Temperature 1600 °F |
|
Haynes Hastelloy® W alloy, gas tungsten arc welds, as-welded Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
MetalTek MTEK 617 Severe Corrosion and Heat Resistant Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
MetalTek MTEK 625 Cast UNS N26625 Severe Corrosion and Heat Resistant Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
MetalTek WCC Cast 105-85 Alloy Steel General structural use.Applications: Cylinders, rolls, hollow shafts.Information provided by MetalTek |
|||
Tensile Strength, Yield | 275 MPa @Strain 0.200 %, Temperature 650 °C |
39900 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes 188 alloy, cold rolled and 1175°C solution annealed sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Yield | 275 MPa @Strain 0.200 %, Temperature 540 °C |
39900 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Hastelloy® B-3® alloy, 6.3 mm plate The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Tensile Strength, Yield | 275 MPa | 39900 psi | Annealed |
Special Metals INCOLOY® Alloy 800 A nickel-iron-chromium alloy with good strength and excellent resistance to oxidation and carburization in high-temperature atmospheres. It also resists corrosion by many aqueous environments. The.. |
|||
Tensile Strength, Yield | 275 MPa | 39900 psi | Annealed |
Special Metals NIMONIC® Alloy 75 A nickel-chromium alloy with good mechanical properties and oxidation resistance at high temperatures. Used for sheet-metal fabrications in gas-turbine engines, for components of industrial furnace.. |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
ThyssenKrupp COR-TEN A Structural Steel This Material Specification applies to plates up to 12.5 mm in thickness made from COR-TEN A.Definition: Weathering means that due to its chemical composition the COR-TEN A steel, when utilized unpr.. |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
ThyssenKrupp FR-30® Fire Resistant Steel With the newly developed FR 30 fire resistant structural steel from TKS there is now the possibility, for the first time, to create steel structures with a fire resistance rating up to F30 without a.. |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
AK Steel ASTM A 570, Grade 40 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
AK Steel ASTM A 907, Grade 40 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |
|||
Tensile Strength, Yield | >= 275 MPa | >= 39900 psi | |
AK Steel ZINCGRIP® 275, Grade 40 Hot Dip Galvanized Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Tensile Strength, Yield | 275 MPa | 39900 psi | Solution Treated (Typical) |
ATI Allegheny Ludlum Altemp® A286 Iron-Base Superalloy, UNS S66286 Allegheny Ludlum Altemp A286 alloy is an iron-base superalloy useful for applications requiring high strength and corrosion resistance up to 704 degrees Celsius and for lower stress applications at .. |
|||
Tensile Strength, Yield | 275 MPa @Strain 0.200 %, Temperature 871 °C |
39900 psi @Strain 0.200 %, Temperature 1600 °F |
|
Haynes 230® alloy, GMAW deposit weld metal Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Tensile Strength, Yield | 275 MPa @Strain 0.200 %, Temperature 538 °C |
39900 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes 230® alloy, cold rolled and 1232°C solution annealed sheet Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |