Tensile Strength, Yield 215 - 450 MPa
31200 - 65300 psi
0.2% proof
Kobe Steel KSTI-1.5AL Alpha Titanium Alloy, Annealed
Nominal Composition: Ti-1.5 Al Applications: Exhaust systems.Features:Heat resistant. Information provided by Kobe Steel
Tensile Strength, Yield 215 MPa

@Strain 0.200 %,
Temperature 980 °C
31200 psi

@Strain 0.200 %,
Temperature 1800 °F
Haynes 25 alloy, cold worked sheet, 20% cold reduction, aged at 595°C (1100°F) for 2 hours
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Yield 215 MPa

@Temperature 870 °C
31200 psi

@Temperature 1600 °F
Haynes Hastelloy® W alloy as a weld filler, base metal Multimet alloy 12.7 mm plate weldment
Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica..
Tensile Strength, Yield 215 MPa

@Strain 0.200 %,
Temperature 649 °C
31200 psi

@Strain 0.200 %,
Temperature 1200 °F
Haynes HR-160® alloy, solution annealed sheet
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Tensile Strength, Yield 215 MPa

@Strain 0.200 %
31200 psi

@Strain 0.200 %
Precipitation Hardened. Value at room temperature
Special Metals INCOLOY® Alloy DS
A nickel-iron-chromium alloy with an addition of silicon. It has good high-temperature strength and excellent resistance to oxidation and carburization. The silicon content makes the alloy resista..
Tensile Strength, Yield 215 MPa
31200 psi
ASTM D638
Solvay TECHNYL® 2912GMH7-P PA66, 63% glass fiber, DRY
Description: Polyamide 66, reinforced with 63% of glass fiber for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2912GMH7-P is used in all sectors of industry, offerin..
Tensile Strength, Yield 215 MPa
31200 psi
ISO 527
Polyram PlusTek RA303G50 Nylon 66 for Injection Molding, 50% Glass Fiber Reinforced, Heat Stabilized, Hydrolysis Resistant
50% Glass fiber reinforced, heat stabilized and hydrolysis resistant Nylon 66 for injection molding applications.Information provided by Polyram.
Copyright © lookpolymers.com All Rights Reserved