Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 26.2 - 141 MPa | 3800 - 20500 psi | Average value: 62.3 MPa Grade Count:15 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Film Tensile Strength at Break, MD | 26.2 - 31.7 MPa | 3800 - 4600 psi | ASTM D882 |
Honeywell ACLAR® CX 130E Heat Sealable PCTFE Film
(discontinued **) Description: ACLAR® CX 130E is a heat sealable PCTFE film with outstanding clarity. It is used where applications require moisture protection.Information provided by Honeywell. |
|||
Film Tensile Strength at Break, MD | 26.2 - 31.7 MPa | 3800 - 4600 psi | ASTM D882 |
Honeywell ACLAR® Cx™ 8A Heat Sealable, Co-Extruded CTFE Film
(discontinued **) Description: ACLAR® Cx™ 8A is a heat sealable coextruded CTFE film.Information provided by Honeywell. |
|||
Film Tensile Strength at Break, MD | 26.2 MPa | 3800 psi | ASTM D882 |
LyondellBasell Petrothene® NA362176 Low Density Polyethylene ApplicationsPETROTHENE NA 362 is a series of low density/EVA copolymers designed for ice bags, bag-in-box, heavy-duty skin packaging and other high strength, easy to seal packaging. NA 362 exhibits.. |
|||
Film Tensile Strength at Break, MD | 26.2 MPa | 3800 psi | ASTM D882 |
LyondellBasell Petrothene® NA362005 Low Density Polyethylene ApplicationsPETROTHENE NA 362 is a series of low density/EVA copolymers designed for ice bags, bag-in-box, heavy-duty skin packaging and other high strength, easy to seal packaging. NA 362 exhibits.. |
|||
Film Tensile Strength at Break, MD | 26.2 MPa | 3800 psi | ASTM-D882 |
Westlake EB171 MDPE Medium Density Polyethylene Westlake EF171 is a MDPE resin suggested for use in shrink packaging applications. This material has good TD shrinkage, good optical properties, excellent machinability, and toughness. This resin gr.. |
|||
Film Tensile Strength at Break, MD | 26.2 MPa | 3800 psi | ASTM D882 |
Westlake EF418 Low Density Polyethylene WESTLAKE polyethylene EF418 is a LDPE formula with excellent optical properties suggested by light and medium duty packaging.Application/UsesLight and medium duty produce bagsClarity packagingGenera.. |
|||
Film Tensile Strength at Break, MD | 26.2 MPa | 3800 psi | ASTM D882 |
Westlake EF796 Low Density Polyethylene Westlake Polyethylene EF796 is a low density formulation suggested for film applications requiring a good balance of properties such as converter film for industrial packaging and general-purpose pa.. |
|||
Film Tensile Strength at Break, MD | 26.2 MPa | 3800 psi | ASTM D882 |
Westlake EF923 Low Density Polyethylene Westlake Polyethylene EF923 is a low density formulation suggested for film applications that require a good balance of properties such as converter film for industrial packaging and general purpose.. |
|||
Film Tensile Strength at Break, MD | 26.2 MPa | 3800 psi | ASTM D882 |
Westlake EN923 Low Density Polyethylene Westlake Polyethylene EN923 is a low density formulation suggested for film applications where enhanced processability and high clarity are required. It is characterized by good tear strength, impa.. |
|||
Film Tensile Strength at Break, MD | 26.2 MPa | 3800 psi | ASTM D882 |
Westlake EP413 Low Density Polyethylene WESTLAKE polyethylene EP413 is a low-density polyethylene recommended for blown or cast film clarity applications. This material has very good optical properties, and is suggested for bakery films ,.. |
|||
Film Tensile Strength at Break, MD | 26.2 MPa | 3800 psi | ASTM D882 |
ExxonMobil LD 317.09 Film Resin LD 317 Series offer excellent impact strength, tensile properties, and heat sealability. Applications include ice bags, frozen food packaging, and other food packaging.Information provided by Exxon.. |
|||
Film Tensile Strength at Break, MD | 26.2 MPa | 3800 psi | ASTM D882 |
ExxonMobil LD 317.87 Film Resin LD 317 Series offer excellent impact strength, tensile properties, and heat sealability. Applications include ice bags, frozen food packaging, and other food packaging.Information provided by Exxon.. |
|||
Film Tensile Strength at Break, MD | 26.2 MPa | 3800 psi | ASTM D882 |
ExxonMobil LDPE LD 151BW Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
Film Tensile Strength at Break, MD | 26.2 MPa | 3800 psi | ASTM D882 |
ExxonMobil LDPE LD 151GZ Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
Film Tensile Strength at Break, MD | 26.2 MPa | 3800 psi | ASTM D882 |
ExxonMobil LDPE LD 151HR Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |