Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 75.2 MPa @Temperature 150 °C |
10900 psi @Temperature 302 °F |
Conditioned; ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Tensile Strength, Yield | 75.2 MPa @Temperature 150 °C |
10900 psi @Temperature 302 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Tensile Strength, Yield | 75.2 MPa @Temperature 23.0 °C |
10900 psi @Temperature 73.4 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Tensile Strength, Yield | 75.0 MPa @Temperature 100 °C |
10900 psi @Temperature 212 °F |
ASTM D638 |
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:.. |
|||
Tensile Strength, Yield | 75.0 MPa @Temperature 250 °C |
10900 psi @Temperature 482 °F |
ASTM D638 |
Gharda Chemicals G-PAEKâ„¢ 1230CF Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 30% carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in .. |
|||
Tensile Strength, Yield | 75.2 MPa @Thickness 1.57 mm |
10900 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP342 Cotton Fabric Description: Fine weave canvas phenolic material with fabric construction weight intermediate to NP310 and NP320. Designed for better machining than grade NP310 and lower cost than NP320.Thickness T.. |
|||
Tensile Strength, Yield | 75.0 MPa @Strain 0.200 %, Temperature 1000 °C |
10900 psi @Strain 0.200 %, Temperature 1830 °F |
|
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Tensile Strength, Yield | 75.2 MPa @Temperature 150 °C |
10900 psi @Temperature 302 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Tensile Strength, Yield | 75.2 MPa @Temperature 150 °C |
10900 psi @Temperature 302 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Tensile Strength, Yield | 75.2 MPa @Temperature 23.0 °C |
10900 psi @Temperature 73.4 °F |
2; ISO 527-2 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Tensile Strength, Yield | 75.2 MPa @Temperature 93.3 °C |
10900 psi @Temperature 200 °F |
90°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 75.0 MPa @Strain 0.200 %, Temperature 1000 °C |
10900 psi @Strain 0.200 %, Temperature 1830 °F |
|
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |