Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 510 MPa @Strain 0.200 % |
74000 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |
|||
Tensile Strength, Yield | 510 MPa @Diameter 12.7 mm, Temperature 25.0 °C |
74000 psi @Diameter 0.500 in, Temperature 77.0 °F |
0.2% offset |
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Tensile Strength, Yield | >= 510 MPa @Strain 0.200 %, Temperature 150 °C |
>= 74000 psi @Strain 0.200 %, Temperature 302 °F |
|
ThyssenKrupp N-A-XTRA® 550 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Tensile Strength, Yield | 510 MPa @Strain 0.200 %, Thickness 9.90 - 25.0 mm |
74000 psi @Strain 0.200 %, Thickness 0.390 - 0.984 in |
Typical Strength |
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m.. |
|||
Tensile Strength, Yield | 510 MPa @Strain 0.200 %, Thickness 152.4 - 203.2 mm |
74000 psi @Strain 0.200 %, Thickness 6.000 - 8.000 in |
Typical Strength |
Constellium Alumold® 500 Rolled Aluminum The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop.. |
|||
Tensile Strength, Yield | >= 510 MPa @Strain 0.200 % |
>= 74000 psi @Strain 0.200 % |
|
Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chrom.. |