Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 450 MPa @Strain 0.200 % |
65300 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 4021 Martensitic Stainless Steel Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 1.00 %, Temperature -196 °C |
65300 psi @Strain 1.00 %, Temperature -321 °F |
EN min.; EN 10002-5 |
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 1.00 %, Temperature -196 °C |
65300 psi @Strain 1.00 %, Temperature -321 °F |
EN min.; EN 10002-5 |
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 1.00 %, Temperature -80.0 °C |
65300 psi @Strain 1.00 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 1.00 %, Temperature -80.0 °C |
65300 psi @Strain 1.00 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms. |
|||
Tensile Strength, Yield | 450 MPa @Strain 1.00 %, Temperature -196 °C |
65300 psi @Strain 1.00 %, Temperature -321 °F |
EN min.; EN 10002-5 |
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 1.00 %, Temperature -196 °C |
65300 psi @Strain 1.00 %, Temperature -321 °F |
EN min.; EN 10002-5 |
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 1.00 %, Temperature -196 °C |
65300 psi @Strain 1.00 %, Temperature -321 °F |
EN min.; EN 10002-5 |
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 0.200 %, Temperature 100 °C |
65300 psi @Strain 0.200 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4501 Duplex Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |
|||
Tensile Strength, Yield | 450 MPa @Strain 1.00 %, Temperature -196 °C |
65300 psi @Strain 1.00 %, Temperature -321 °F |
EN min.; EN 10002-5 |
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 0.200 % |
65300 psi @Strain 0.200 % |
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu SAF 2304® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 0.200 %, Temperature 100 °C |
65300 psi @Strain 0.200 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 0.200 %, Thickness 1.45 mm |
65300 psi @Strain 0.200 %, Thickness 0.0571 in |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 0.200 %, Thickness 240 - 305 mm |
65300 psi @Strain 0.200 %, Thickness 9.45 - 12.0 in |
Typical Strength |
Constellium Certal® SPC Aluminum Certal® SPC has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property in man.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 0.200 %, Thickness 160 - 180 mm |
65300 psi @Strain 0.200 %, Thickness 6.30 - 7.09 in |
Typical Strength |
Constellium Fortal® Aluminum Alloy Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m.. |
|||
Tensile Strength, Yield | 450 MPa @Strain 0.200 % |
65300 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu LDX 2101® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |