Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 355 MPa @Strain 1.00 %, Temperature -80.0 °C |
51500 psi @Strain 1.00 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 355 MPa @Strain 1.00 %, Temperature -80.0 °C |
51500 psi @Strain 1.00 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 355 MPa @Strain 1.00 %, Temperature -80.0 °C |
51500 psi @Strain 1.00 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 355 MPa @Strain 1.00 %, Temperature -80.0 °C |
51500 psi @Strain 1.00 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 355 MPa @Strain 1.00 %, Temperature -80.0 °C |
51500 psi @Strain 1.00 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 355 MPa @Strain 1.00 %, Temperature -80.0 °C |
51500 psi @Strain 1.00 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Tensile Strength, Yield | 355 MPa @Strain 0.200 % |
51500 psi @Strain 0.200 % |
Typical |
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water .. |
|||
Tensile Strength, Yield | 355 MPa @Thickness 12.7 mm, Temperature 427 °C |
51500 psi @Thickness 0.500 in, Temperature 801 °F |
0.2% Offset |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Tensile Strength, Yield | >= 355 MPa @Thickness 16.0 mm |
>= 51500 psi @Thickness 0.630 in |
|
ThyssenKrupp COR-TEN B Structural Steel This Material Specification applies to plates up to 50 mm in thickness made from COR-TEN B.Definition: Weathering means that due to its chemical composition the COR-TEN B steel, when utilized unprot.. |
|||
Tensile Strength, Yield | 355 MPa @Strain 0.200 %, Thickness 15.0 - 35.0 mm |
51500 psi @Strain 0.200 %, Thickness 0.591 - 1.38 in |
Typical Strength |
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing .. |
|||
Tensile Strength, Yield | 355 MPa @Strain 0.200 %, Thickness 80.0 - 120 mm |
51500 psi @Strain 0.200 %, Thickness 3.15 - 4.72 in |
Typical Strength |
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing .. |