Category Metal , Ferrous Metal , Alloy Steel , Carbon Steel , Low Carbon Steel
Manufacturer ThyssenKrupp
Trade Name COR-TEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ThyssenKrupp COR-TEN B Structural Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This Material Specification applies to plates up to 50 mm in thickness made from COR-TEN B.Definition: Weathering means that due to its chemical composition the COR-TEN B steel, when utilized unprotected, exhibits increased resistance to atmospheric corrosion compared to unalloyed steels. This is because it forms a protective layer on its surface under the influence of the weather. The layer protecting the surface develops and regenerates continuously when subjected to the influence of the weather. In general the covering layer offers protection against atmospheric corrosion in industrial, urban and country-side climate. In cases of particular air pollution by aggressive agents conventional surface protection is recommended. Coating is absolutely necessary in cases of contact with water for long periods, when permanently exposed to moisture, or if it is to be used in the vicinity of the sea. The susceptibility of paint coats to undercreepage by rust is less in the case of weathering steel than in the case of comparable non-weathering steel.Application: The steel is used for various types of welded, bolted and riveted constructions e.g. steel frame structures, bridges, tanks and containers, exhaust systems, vehicles and equipment constructions.Information Provided by Thyssen Krupp
Mechanical Properties Metric English Comments
Tensile Strength at Break 470 - 630 MPa

@Thickness 16.0 mm
68200 - 91400 psi

@Thickness 0.630 in
470 - 630 MPa

@Thickness 16.0 - 50.0 mm
68200 - 91400 psi

@Thickness 0.630 - 1.97 in
Tensile Strength, Yield >= 345 MPa

@Thickness 16.0 - 50.0 mm
>= 50000 psi

@Thickness 0.630 - 1.97 in
>= 355 MPa

@Thickness 16.0 mm
>= 51500 psi

@Thickness 0.630 in
Elongation at Break 20 %

@Thickness 16.0 mm
20 %

@Thickness 0.630 in
20 %

@Thickness 16.0 - 50.0 mm
20 %

@Thickness 0.630 - 1.97 in
Charpy Impact 27.0 J

@Thickness 10.0 mm,
Temperature -20.0 °C
19.9 ft-lb

@Thickness 0.394 in,
Temperature -4.00 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.16 %
<= 0.16 %
Chromium, Cr 0.40 - 0.65 %
0.40 - 0.65 %
Copper, Cu 0.25 - 0.40 %
0.25 - 0.40 %
Manganese, Mn 0.80 - 1.25 %
0.80 - 1.25 %
Nickel, Ni <= 0.40 %
<= 0.40 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si 0.30 - 0.50 %
0.30 - 0.50 %
Sulfur, S <= 0.030 %
<= 0.030 %
Vanadium, V 0.020 - 0.10 %
0.020 - 0.10 %