Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 302 x 10-8 mm³/N-M | 150 x 10-10 in³-min/ft-lb-hr | |
Quadrant EPP Ketron® CA30 LSG PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
K (wear) Factor | 302 x 10-8 mm³/N-M | 150 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Ketron® CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
K (wear) Factor | 302 x 10-8 mm³/N-M | 150 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Technetics Group Amicon™ PEEK 30% Carbon
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
K (wear) Factor | 302 x 10-8 mm³/N-M | 150 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Duratron® PAI T4501 Polyamide-imide, compression molded bearing grade (ASTM Product Data Sheet) |
|||
K (wear) Factor | 302 x 10-8 mm³/N-M | 150 x 10-10 in³-min/ft-lb-hr | QTM55010 |
Quadrant EPP Duratron® PI D7000 PI Unfilled Polyimide (ASTM Product Data Sheet) |
|||
K (wear) Factor | 302 - 1010 x 10-8 mm³/N-M | 150 - 500 x 10-10 in³-min/ft-lb-hr | Average value: 637 x 10<sup>-8</sup> mm³/N-M Grade Count:4 |
Overview of materials for Polyamide-Imide, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
K (wear) Factor | 302 x 10-8 mm³/N-M | 150 x 10-10 in³-min/ft-lb-hr | |
Greene Tweed Avalon® 7 PTFE, Pigmented and Molybdenum Filled Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin.. |
|||
K (wear) Factor | 302 x 10-8 mm³/N-M | 150 x 10-10 in³-min/ft-lb-hr | K=W/PVT where W=wear (inches^3); P=applied pressure (psi); V=velocity (fpm); T=time (hours). |
A. Schulman ComAlloy Lubrilon® 602 Nylon 6/6, Molybdenum Disulfide Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |