Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 22.2 x 10-8 mm³/N-M | 11.0 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP BX03658N SAN LNP* LUBRICOMP* BX03658N is a compound based on SAN resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerances, good for Water Meter A.. |
|||
K (wear) Factor | 22.2 x 10-8 mm³/N-M | 11.0 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DFL14 PC LNP LUBRICOMP* DFL14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
K (wear) Factor | 22.2 x 10-8 mm³/N-M | 11.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP 9X06483 PA 46 LNP* Lubricomp* 9X06483 is a compound based on a Nylon 4/6 containing PTFE. Added feature of this grade is: Heat Stabilized. |
|||
K (wear) Factor | 22.2 x 10-8 mm³/N-M | 11.0 x 10-10 in³-min/ft-lb-hr | Lubricated: 0.375 m/s, 6.9 MPa (75 fpm, 1000 psi); ASTM D3702 |
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon PAI has the h.. |
|||
K (wear) Factor | 22.2 x 10-8 mm³/N-M | 11.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubricomp IP003 PA6.12 LNP* Lubricomp* IP003 is a Nylon 6/12 base resin containing PTFE and Silicone.This data was supplied by SABIC-IP for the Americas region. |
|||
K (wear) Factor | 22.2 x 10-8 mm³/N-M | 11.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP KL003 Acetal Copolymer LNP LUBRICOMP* KL003 is a compound based on Acetal Copolymer resin containing 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
K (wear) Factor | 22.2 x 10-8 mm³/N-M | 11.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopoly (Asia Pacific) LNP* Lubricomp* KP003AXZ is a compound based on Acetal Homopolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 22.2 x 10-8 mm³/N-M | 11.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopolymer LNP* LUBRICOMP* KP003AXZ is a compound based on Acetal Homopolymer resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
K (wear) Factor | 22.2 x 10-8 mm³/N-M | 11.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA 6/10 (Asia Pacific) LNP* Lubricomp* QAP22S is a compound based on Nylon 6/10 resin containing PTFE, Aramid Fiber, Silicone. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
K (wear) Factor | 22.2 x 10-8 mm³/N-M | 11.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA6.10 LNP* LUBRICOMP* QAP22S is a compound based on Nylon 6/10 resin containing 10% PTFE/Silicone, 10% Aramid Fiber. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
K (wear) Factor | 22.2 x 10-8 mm³/N-M | 11.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 LNP* LUBRICOMP* RFP36 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE, Silicone. Added features of this material include: Wear Resistant. |
|||
K (wear) Factor | 22.2 x 10-8 mm³/N-M | 11.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 (Asia Pacific) LNP* Lubricomp* RFP36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. This product is also known as Lub.. |
|||
K (wear) Factor | 22.2 x 10-8 mm³/N-M | 11.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFP36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. |
|||
K (wear) Factor | 22.2 x 10-8 mm³/N-M | 11.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFP36S PA 66 LNP* LUBRICOMP* RFP36S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
K (wear) Factor | 22.2 x 10-8 mm³/N-M | 11.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFP36XXZ PA 66 (Asia Pacific) LNP Lubricomp RFP36XXZ is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: internally lubricated. Also known as Lubricomp RFL-4536 .. |
|||
K (wear) Factor | 22.2 x 10-8 mm³/N-M | 11.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS LNP* LUBRICOMP* ZL003 is a compound based on PPE+PS resin containing 15% PTFE. Added features of this material include: Wear Resistant. |
|||
K (wear) Factor | 22.2 x 10-8 mm³/N-M | 11.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS (Asia Pacific) LNP LUBRICOMP ZL003 is a compound based on PPE+PS Blend resin containing PTFE. Added features of this material include:internally Lubricated. Also known as LUBRICOMP ZL-4030 |
|||
K (wear) Factor | 22.2 x 10-8 mm³/N-M | 11.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubricomp XL004 Amorphous Polyamide LNP* Lubricomp* XL-4040 is a compound based on Amorphous Nylon, containing PTFE.This data was supplied by SABIC-IP for the Americas region. |