Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 151 x 10-8 mm³/N-M | 75.0 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Duratron® T7130 PAI Polyamide-imide, carbon fiber reinforced, extruded (ASTM Product Data Sheet) |
|||
K (wear) Factor | 151 x 10-8 mm³/N-M | 75.0 x 10-10 in³-min/ft-lb-hr | 40psi, 50ft/min; tested in accordance with LNP WI-0687 |
LNP Thermocomp® EC-1006 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
K (wear) Factor | 151 x 10-8 mm³/N-M | 75.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
K (wear) Factor | 151 x 10-8 mm³/N-M | 75.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI (Asia Pacific) LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
K (wear) Factor | 151 x 10-8 mm³/N-M | 75.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP THERMOCOMP EC006E PEI LNP THERMOCOMP* EC006E is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive |
|||
K (wear) Factor | 151 x 10-8 mm³/N-M | 75.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP THERMOCOMP RF006H PA 66 LNP THERMOCOMP* RF006H is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
K (wear) Factor | 151 x 10-8 mm³/N-M | 75.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP THERMOCOMP RF006XXZ PA 66 LNP THERMOCOMP* RF006XXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber |