Category Polymer , Thermoplastic , Polyamide-imide (PAI) , Polyamide-Imide, Graphite Filled
Manufacturer Quadrant Engineering Plastics Products
Trade Name Duratron® T7130
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Duratron® T7130 PAI Polyamide-imide, carbon fiber reinforced, extruded (ASTM Product Data Sheet).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Water Absorption 0.30 %
0.30 %
Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 1.5 %
1.5 %
Immersion; ASTM D570(2)
Mechanical Properties Metric English Comments
Hardness, Rockwell E 91
91
ASTM D785
Tensile Strength 152 MPa
22000 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Tensile Modulus 8.27 GPa
1200 ksi
ASTM D638
Compressive Strength 255 MPa
37000 psi
10% Def.; ASTM D695
Compressive Modulus 6.89 GPa
1000 ksi
ASTM D695
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256 Type A
Coefficient of Friction, Dynamic 0.30
0.30
Dry vs. Steel; QTM 55007
Coefficient of Friction, Static 0.30
0.30
QTM 55007
K (wear) Factor 151 x 10-8 mm³/N-M
75.0 x 10-10 in³-min/ft-lb-hr
QTM 55010
Limiting Pressure Velocity 0.490 MPa-m/sec
14000 psi-ft/min
4:1 safety factor; QTM 55007
Thermal Properties Metric English Comments
CTE, linear 9.00 µm/m-°C

@Temperature -40.0 - 149 °C
5.00 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.519 W/m-K
3.60 BTU-in/hr-ft²-°F
ASTM F433
Maximum Service Temperature, Air 260 °C
500 °F
Long Term
Deflection Temperature at 1.8 MPa (264 psi) 282 °C
540 °F
ASTM D648
Glass Transition Temp, Tg 275 °C
527 °F
ASTM D3418
Flammability, UL94 V-0
V-0
1/8 inch (Estimated Rating)
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 1e+13 ohm
<= 1e+13 ohm
EOS/ESD S11.11
Compliance Properties Metric English Comments
3A-Dairy No
No
Canada AG No
No
FDA No
No
NSF No
No
USDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Limited
Limited
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Limited
Limited
Chlorinated Solvents Acceptable
Acceptable
Conductive / Static Dissipative No
No
Continuous Sunlight Acceptable
Acceptable
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Descriptive Properties Value Comments
Machinability 8
1-10, 1=Easier to Machine