Mechanical Properties Metric English Comments
Tensile Strength at Break 211 MPa

@Temperature 23.0 °C
30600 psi

@Temperature 73.4 °F
ISO 527-2
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include ..
Tensile Strength at Break 211 MPa

@Temperature 23.0 °C
30600 psi

@Temperature 73.4 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry)
Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre..
Tensile Strength at Break 211 MPa

@Temperature 23.0 °C
30600 psi

@Temperature 73.4 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp..
Tensile Strength at Break 211 MPa

@Temperature 23.0 °C
30600 psi

@Temperature 73.4 °F
ISO 527-2
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength..
Tensile Strength at Break 211 MPa

@Temperature 23.0 °C
30600 psi

@Temperature 73.4 °F
ISO 527-2
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer
Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp..