Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C4210 PC+ABS (Europe-Africa-Middle East) CYCOLOY C4210 is a 10% glass reinforced, non-FR PC+ABS grade. It shows high heat resistance, excellent strength and rigidity with good cosmetic appearance. It combines a good processabity with a low.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Nilit Nilamid A G7 FR PH1 35% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G7 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a UL 94 V0 listing 1.5 and a complete yellow card. The formulation has been optim.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Asia Pacific) High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® LR180R PC (Europe-Africa-Middle East) LR180R is a medium viscosity,release containing multipurpose polycarbonate industrial gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Nilit Nilamid A G10 FR PH1 50% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G10 FR PH1 was developed specifically for highly loaded, structural applications in the electrical industry. It combines extremely high mechanical performance with flame retar.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 4301 PPC+PC Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6
(Unverified Data**) Zytel® 73G30HSL NC010 is a 30% glass fiber reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
ISO 80 |
LG Chemical LG-709 ABS, Low Gloss, Super High Heat Resistance Information Provided by LG Chem |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
Styron MAGNUM™ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low .. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
Styron Magnumâ„¢ 3513 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3513 is a grade which combines high impact with good flowability. It is suitable for injection molding and extrusion applications.Information provided by DowThis product line was spun .. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXAMID 126F6RY01 Nylon 6, 30% Glass Fiber SAXAMID 126F6RY01 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Europe-Africa-Middle East) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp RF00AES PA 66 (Europe-Africa-Middle East) LNP THERMOCOMP* RF00AES is a compound based on PA66 resin containing Glass Fiber, Mold Release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -40.0 °C |
5.23 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp RF00AES PA 66 (Europe-Africa-Middle East) LNP THERMOCOMP* RF00AES is a compound based on PA66 resin containing Glass Fiber, Mold Release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Borealis GB364WG Polypropylene Compound, Glass Fiber Reinforced GB364WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Borealis GB366WG Polypropylene Compound, Glass Fiber Reinforced GB366WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4 sp=62; ISO 180/1A |
Eurostar Staramide BG6H PA6, 30% Glass Filled, Injection Molded BG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide BG7HU PA6, 35% Glass Fiber Filled, Heat and UV Stabilized, Injection Molded Staramide BG7H is a Heat and UV Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 179/1eA |
Eurostar Staramide RF00AES PA66/6, 50% Glass Filled, Injection Molded Staramide RF00AES is a 50% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 50V S3)Information provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR50 BK009 MX01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, improved impact, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 GR20 NL XA70 PA6, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, Conditioned Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R530H BK0202 Nylon 66, 30% Glass Reinforced, Conditioned Vydyne® R530H BK0202 is general-purpose, recycled, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the rete.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, Conditioned Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612
(Unverified Data**) Zytel® FG77G33L NC010 is a 33% glass fiber reinforced polyamide 612 resin for injection molding. It has been developed for consideration for applications such as parts in the food industry.Informat.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Europe-Africa-Middle East) Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, Conditioned Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh.. |