Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Nilit Nilamid B3N Unfilled, Nucleated PA6 Description: Nilamid B3N is an unfilled, nucleated NYLON 6. It is fast cycling, and combines ease of processing with good overall mechanical characteristics.Key characteristics: Fast cyclingEasy pro.. |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
DuPont Performance Polymers Crastin® FG6129 NC010 PBT
(Unverified Data**) Crastin® FG6129 NC010 is an unreinforced, high viscosity polybutylene terephthalate resin for extrusion and injection molding. It has been developed for consideration into applications such as part.. |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Eastman 9921 PET Injection Molded
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Thickness 3.17 mm, Temperature -40.0 °C |
2.14 ft-lb/in² @Thickness 0.125 in, Temperature -40.0 °F |
ISO 180 |
Phillips Sumika Marlex® ABF-300 High Flow Thermoplastic Olefin
(discontinued **) Applications: Automotive exterior fasciasInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66 Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a.. |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-3250 42% Chalk-Filled Polypropylene Homopolymer INNOPOL® CS 1-3250 is a 42% chalk-filled polypropylene homopolymer compound /PP-H KD42 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 1-3250 is developed f.. |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature -40.0 °C |
2.14 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
LyondellBasell Hostacomâ„¢ CB267 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CB267 medium melt flow, 1,600 MPa flexural modulus thermoplastic elastomeric olefin (TEO) resin has an excellent balance of scratch and mar resistance, rigidity and impac.. |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 180/1A |
Borealis Daplen™ EF005AE Polypropylene TPO Compound Daplen™ EF005AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 180/1A |
Borealis Daplen™ EF261AI Polypropylene TPO Compound Daplen™ EF261AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Polyram PlusTek PB340S50 Nylon 6 for Injection Molding, 50% Glass-beads Reinforced, Heat Stabilized 50% Glass-beads reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 180 |
Total PPC 11750 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11750 is a nucleated and controlled-rheology heterophasic copolymer with very high Melt Flow index of 50 g/10 min.Polypropylene PPC 11750 is characterized by good impact resistance.. |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Eastman Eastar EN001 Copolyester Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming pro.. |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature 0.000 °C |
2.14 ft-lb/in² @Temperature 32.0 °F |
ISO 180/1A |
Domo 2348M Polypropylene Copolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610
(Unverified Data**) Zytel® RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredient by weight. It is an unreinforced, heat stabilized, lubricated black grad.. |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature -40.0 °C |
2.14 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
BASF Nypel® 2351 HS BK PA6 (Dry) Description: Nypel® 2351 HS BK is a heat stabilized, pigmented black, impact modified PA6 extrusion grade compound. Quality and performance are combines at a lower cost. It is based on recycled PA6.. |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Eastman 9921W PET Injection Molded
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612
(Unverified Data**) Zytel® SC315 NC010 is an unreinforced, lubricated 612 polyamide suitable for injection molding. It has been developed for applications such as parts for the healthcare industry.Information provided.. |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612
(Unverified Data**) Zytel® SC315 NC010 is an unreinforced, lubricated 612 polyamide suitable for injection molding. It has been developed for applications such as parts for the healthcare industry.Information provided.. |
|||
Izod Impact, Notched (ISO) | 4.50 kJ/m² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry) Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF |