Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS PC+ABS Recycle Resin with good flow, good temperature resistance and moderate impact |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® RCY6713 PC (Asia Pacific) Cycoloy* RCY6713 resin is an injection moldable high heat PC blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1.5.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics GELOY HRA170D ASA+PC (Europe-Africa-Middle East) GELOY HRA170D resin is a PC-ASA blend with permanent antistatic behavior. It is typically used in applications that require antidust properties and high impact retention. Geloy HRA170D resin is typi.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics GELOY HRA222 ASA (Asia Pacific) GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. Use for exterior/interior electrical applications requiring UV resistance. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Europe-Africa-Middle East) Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant ASA-PC alloy for injection moulding processes. This grade has a F1 rating according UL746C. Typical properties as measured.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible, Easy Moldi.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Total Lacqtene® 2003 PBK 41 HDPE pipe, sheet
(discontinued **) LACQTENE® 2003 PBK 41 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2003 PBK 41 is a black compound especially developed for i.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DFI14 PC LNP* Lubricomp* DFI14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 2% Silicone. Added features include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC (Asia Pacific) LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® C 246 V 30 PA6, 30% glass fiber, DRY Description: Polyamide PA6, reinforced with 30 % of glass fiber, high impact strength, for injection molding.Available in: Asia Pacific and North AmericaProduct Applications: Having good mechanical .. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, DRY Description TECHNYLSTARâ„¢ AFX 218 V50 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is availab.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4mm, Cut; ISO 180/1A |
SABIC Innovative Plastics SABIC STAMAX 40YM240 PP SABIC® STAMAX 40YM240 is a 40% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 16497161... |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER (Asia Pacific) PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP PF008S PA 6 LNP THERMOCOMP* PF008S is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PX1112 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1112 is an unfilled medium heat resistant material. This grade offers improved impact resistance to meet the ECE-dashboard standard. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP PF008 PA 6 (Asia Pacific) LNP THERMOCOMP* PF008 is a compound based on Nylon 6 resin containing Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP PF008QS PA 6 LNP THERMOCOMP* PF008QS is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized, Reduced Moisture. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PX0844 PPE+PS PPE+PS blend. Unfilled. UL94 HB rated. Low water absorption. Hydrolytic stability. Dimensional stability. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GF60-66/6 XE-NBK1 60% Glass Fiber Reinforced, Engineering Grade Nylon 66/6 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO 180 |
Polyram RamTough PZ509 Polycarbonate, Easy Flow, Flame Retardant Non-transparent polycarbonate, easy flow, flame retardant, for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO 180 |
Polyram RamTough PZ513 Polycarbonate, Easy Flow, Flame Retardant Transparent polycarbonate, UV stabilized, easy flow, flame retardant, for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® 70G30HSL NC010 Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -40.0 °C |
8.09 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® ST801AHS BK010 Nylon 66
(Unverified Data**) Super Toughened Heat Stabilized Polyamide 66 Zytel ST801AHS BK010 is a Super Tough high performance black polyamide 66 resin. It offers outstanding molding performance in injection molding applicati.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -40.0 °C |
8.09 ft-lb/in² @Temperature -40.0 °F |
ISO Test |
BASF Ultramid® B3ZG7 OSI BK23273 35% Glass Filled PA6 (Dry) Ultramid B3ZG7 OSI BK23273 is a 35% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet demanding mechanical and chemical requi.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO Test |
BASF Ultramid® 1603-2 NF2004 43% Glass Filled PA66 (Conditioned) Ultramid 1603-2 NF2004 is a 43% glass reinforced, heat stabilized injection molding nylon 6/6 with the highest level of glass reinforcement for maximum strength and stiffness. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® LM70G35HSLX BK314 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Laser Markable Polyamide 66 Zytel LM70G35HSLX is a 35% glass fiber reinforced heat stabilized lubricated polyamide 66 for injection molding. It is well suited fo.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PX2355 PPE+HIPS (Europe-Africa-Middle East) NORYL PX2355 is an unfilled, medium heat, low odour and low emission material with excellent heat aging performance. It has been developed for automotive interior applications, such as instrument pa.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® B3WG5 BK 00564 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |