Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 4.04 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 8.50 - 9.00 kJ/m²
4.04 - 4.28 ft-lb/in²
ASTM D256
Polikim EFALON® K-25 PTFE, 25% Carbon Filled
K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings...
Izod Impact, Notched (ISO) 8.50 - 14.0 kJ/m²
4.04 - 6.66 ft-lb/in²
Average value: 11.9 kJ/m² Grade Count:4
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..
Izod Impact, Notched (ISO) 8.50 kJ/m²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
DuPont Performance Polymers Rynite® FR530L BK507 PET  (Unverified Data**)
Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO 180
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic..
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO 180
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In..
Izod Impact, Notched (ISO) 8.50 - 57.0 kJ/m²
4.04 - 27.1 ft-lb/in²
Average value: 18.0 kJ/m² Grade Count:10
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Izod Impact, Notched (ISO) 8.50 kJ/m²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
MBA Polymers PS 3122 Post-consumer recycled impact modified polystyrene
Available in standard black.Information provided by MBA Polymers.
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
Type 1, Notch A; ISO 180
Solvay Specialty Polymers Amodel® AS-1935 HS Polyphthalamide (PPA), 35% Glass Fiber
Amodel® AS-1935 HS is a 35% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e..
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO 180
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining..
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO 180
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber
AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch..
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO 180
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide..
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO 180
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber
KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical..
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
Notch A; ISO 180
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber
Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low ..
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO 180
Tisan TISESTER® 30% Glass Fiber Reinforced Heat Stabilized Copolymer Polybutylene Terephthalate
TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi..
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO 180-93
Wellman Wellamid® GF10-66/6-LI6-NBK4 10% Glass Reinforced, Toughened Nylon 66/6
Description: Glass Reinforced, Toughened Nylon 66/6Information provided by Wellman.
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO 180
Polyram PlusTek RA300G7 Nylon 6.6 for Injection Molding, 35% Glass Fiber Reinforced, Heat Stabilized
Heat stabilized, 35% glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram.
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO 180
Total PPC 12712 Polypropylene, Heterophasic Copolymer
ATOFINA Propylene 12712 is a nucleated controlled-rheology heterophasic copolymer. PPC 12712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h..
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO 180/1A
Addiplast Addinyl A2I V25 Flame Retardant Nylon 66, 25% Glass Filled
Flame retardant, 25% glass fiber reinforced, halogen freeInformation provided by Addiplast.
Izod Impact, Notched (ISO) 8.50 kJ/m²

@Temperature -40.0 °C
4.04 ft-lb/in²

@Temperature -40.0 °F
ISO Test
BASF Petra® 130 BK-112 30% Glass Filled PET
Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength ..
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO Test
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Dry)
Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature performance and ..
Izod Impact, Notched (ISO) 8.50 kJ/m²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Dry)
Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO 180/1A
Addiplast Addinyl B2I V25 Flame Retardant Nylon 6, 25% Glass Filled
Flame retardant, 25% glass fiber reinforced, halogen freeInformation provided by Addiplast.
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO 180/A
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Conditioned)
Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability.
Izod Impact, Notched (ISO) 8.50 kJ/m²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Conditioned)
Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele..
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO 180/1A
Total Lacqrene® 6631 Impact Polystyrene  (discontinued **)
LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application..
Izod Impact, Notched (ISO) 8.50 - 12.0 kJ/m²
4.04 - 5.71 ft-lb/in²
Average value: 10.2 kJ/m² Grade Count:8
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..
Copyright © lookpolymers.com All Rights Reserved