Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 5.80 - 9.60 kJ/m² | 2.76 - 4.57 ft-lb/in² | Average value: 7.75 kJ/m² Grade Count:6 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched (ISO) | 5.80 kJ/m² | 2.76 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re.. |
|||
Izod Impact, Notched (ISO) | 5.80 kJ/m² | 2.76 ft-lb/in² | Sample Type A; ISO 180:2000 |
Global EPP PA 6C OFN Cast Polyamide 6 + Blended Liquid Lubricant Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Izod Impact, Notched (ISO) | 5.80 kJ/m² | 2.76 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® ST35G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Izod Impact, Notched (ISO) | 5.80 kJ/m² | 2.76 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK) AV-742 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wea.. |
|||
Izod Impact, Notched (ISO) | 5.80 kJ/m² | 2.76 ft-lb/in² | 1A; ISO 180 |
Azoty Tarnow™ TARNOFORM 300 GF2 POM 10% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Izod Impact, Notched (ISO) | 5.80 kJ/m² | 2.76 ft-lb/in² | 1A; ISO 180 |
Azoty Tarnow™ TARNOFORM 300 GF3 POM 15% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Izod Impact, Notched (ISO) | 5.80 kJ/m² | 2.76 ft-lb/in² | 1A; ISO 180 |
Azoty Tarnow™ TARNOFORM 500 GF6 POM 30% glass fiber reinforced, high flow injection molding grade, suitable for applications where high strength and stiffness is required, combined with higher flowability during molding.Information pr.. |
|||
Izod Impact, Notched (ISO) | 5.80 kJ/m² | 2.76 ft-lb/in² | ISO Test |
BASF Ultramid® 8266G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8266G HS is a heat stabilized, 40% glass and mineral reinforced nylon 6 injection molding compound resulting in a balance of engineering properties with excellent dimensional stability, low.. |
|||
Izod Impact, Notched (ISO) | 5.80 kJ/m² | 2.76 ft-lb/in² | ISO Test |
BASF Ultramid® SEGM35 H1 BK-126 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid SEGM35 H1 BK-126 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compared to 8267G .. |