Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C7410 PC+ABS (Asia Pacific) Cycoloy* C7410 resin is a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | ISO 180 |
Phillips Sumika Marlex® CHP-370 Thermoplastic Polyolefin
(discontinued **) Thermoplastic Polyolefin, Good Stiffness and Impact PerformanceApplications: Automotive Pillar TrimConditioning after Molding: 48 hr at 23°CNominal Shrinkage: 0.8-1.0%Drying conditionsTemperature: .. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | ISO 180 |
Iran Petrochemical (PCC) SV-0157 Acrylonitrile Butadiene Styrene SV - 0157 ABS extrusion grade has been formulated to provide excellent mechanical properties, extrusion stability, vacuum formability and chemical resistance. It has low flow with high impact streng.. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC (Asia Pacific) LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² @Temperature 0.000 °C |
14.8 ft-lb/in² @Temperature 32.0 °F |
80*10*4mm, Cut; ISO 180/1A |
SABIC Innovative Plastics SABIC PPCOMPOUND 8620A PP SABIC® PPcompound 8620A is a mineral filled, impact modified polypropylene TPO. It was originally designed for painted automotive bumper fascia applications where a combination of good flow, hig.. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRILOY D20001 PPO LNP* LUBRILOY* Z20001 is a compound based on PPO resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® IQ357 PBT+PC Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® IQ357M PBT+PC Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Asia Pacific) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® IQ357U PBT+PC Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Asia Pacific) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP C7410 PC+ABS (Asia Pacific) LNP* Thermocomp* C7410 compound is a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP 2X00858 FP-F (FEP) LNP* THERMOCOMP* 2X00858 is a compound based on FEP resin containing proprietary fillers. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP TF002 PU LNP* THERMOCOMP* TF002 is a compound based on Polyurethane resin containing 10% Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² @Temperature 23.0 °C |
14.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Verton OV00A PPS (Asia Pacific) LNP* Verton* OV00A is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | ISO 180/1A |
Chi Mei Polylac® PA-709 ABS Super impact |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | ISO 180/1A |
Chi Mei Polylac® PA-709S ABS - Extrusion Super Impact Extrusion |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | 1A; ISO 180 |
Azoty Tarnow™ TARNOFORM 200 HI4 POM Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRILOY Z20001 PPO LNP* Lubriloy* Z20001 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² @Temperature 23.0 °C |
14.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Verton OV00A PPS LNP* Verton* OV00A is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON PX00700 PA 6 LNP VERTON* PX00700 is a compound based on Nylon 6 resin containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Izod Impact, Notched (ISO) | 31.0 kJ/m² | 14.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON PX00700 PA 6 (Asia Pacific) LNP* Verton* PX00700 is a compound based on Nylon 6 resin containing Long Glass Fiber. |