Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) SV-0157 Acrylonitrile Butadiene Styrene

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) SV-0157 Acrylonitrile Butadiene Styrene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
SV - 0157 ABS extrusion grade has been formulated to provide excellent mechanical properties, extrusion stability, vacuum formability and chemical resistance. It has low flow with high impact strength at ambient temperature and considerable impact strength at low temperatures. This grade has a wide processing window.Applications: SV-0157 extrusion grade is mainly used for parts which need significant impact resistance. Since sheets can be vacuum–formed, it is the appropriate grade for refrigerator sheets which are in direct contact with rigid insulating foam produced with cyclo-pentane as blowing agent.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Melt Flow 0.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
ASTM D785
Tensile Strength, Yield 45.1 MPa
6540 psi
ASTM D638
Elongation at Break 70 %
70 %
ASTM D638
Flexural Yield Strength 61.8 MPa
8960 psi
ASTM D790
Flexural Modulus 2.15 GPa
312 ksi
ASTM D790
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 100.5 °C
212.9 °F
ASTM D1525
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: