Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS PC+ABS Blend with 10% Glass Reinforce. High flow, High heat resistance., Excellent balance strength/rigidity. Good impact/appearance. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® HFD4413 PC Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® ZLL12CP PC (Europe-Africa-Middle East) Medium viscosity general purpose flame retardant polycarbonate grade based on recycled material. Rated UL94 V2 at 1.5 mm. Limited color availability. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® ML3999 PC (Europe-Africa-Middle East) LEXAN ML3999 is a medium viscosity, 20% glass reinforced grade. It offers excellent flame retardancy and is especially designed for applications requiring high rigidity together with high heat. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI (Asia Pacific) LNP* Lubricomp* EX06405 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM 2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM 2100R PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM 2110 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM 2200F PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WL003 is a compound based on Polybutylene Terephalate resin containing PTFE. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT LNP LUBRICOMP* WL004 is a compound based on PBT resin containing 20% PTFE. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DE0026 PC (Europe-Africa-Middle East) LNP* Stat-kon* DC-1002 FR is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Flame Retardant, Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DEL13PXC PC (Europe-Africa-Middle East) LNP* Stat-kon* DEL13PXC is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Superior Molding. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® DR51 PBT (Europe-Africa-Middle East) VALOX DR51 is a 15% glass fiber reinforced PBT injection moulding resin with excellent mechanical, thermal and electrical performance. Applications: spotlights, appliance housings, handles. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® SHF4340 PBT (Europe-Africa-Middle East) 20% GF Super High Flow PBT |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon WC003 PBT (Europe-Africa-Middle East) LNP* Stat-kon* WC003 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP EC004XXC PEI LNP* THERMOCOMP* EC004XXC is a compound based on Polyetherimide resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP MF003SU PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MF003SU is a compound based on polypropylene resin containing Glass Fiber. Added features include : Heat Stabilized, UV-Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP NF0061 PC+ABS (Europe-Africa-Middle East) LNP* THERMOCOMP* NF0061 is a compound based on PC+ABS resin containing Glass Fiber, Flame Retardant. Added features include : Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12 (Asia Pacific) Glass filled Nylon 12 |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide RFB53U PA66, 50% Glass Bead/Fiber Filled, Injection Molded RFB53U is a Glass Bead/ Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 1525 VK Z4)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® HFD4413 PC (Europe-Africa-Middle East) Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Asia Pacific) NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing 20% Glass Bead, 15% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retard.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL FE1630PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1630PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | ISO 180/U |
Victrex® PEEK 150FC30 Easy Flow Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy .. |