Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral filled PA6 non-halogen FR compound |
|||
Izod Impact, Unnotched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP CX05031 PS (Europe-Africa-Middle East) LNP* Lubricomp* CX05031 is a compound based on Polystyrene resin containing Graphite, Silicone. Added features include; Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 5.00 - 10.0 kJ/m² | 2.38 - 4.76 ft-lb/in² | Average value: 7.57 kJ/m² Grade Count:10 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Izod Impact, Unnotched (ISO) | >= 5.00 kJ/m² | >= 2.38 ft-lb/in² | ISO 180/1A |
Iran Petrochemical (PCC) Tabriz 6630/1 High Impact Polystyrene
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Izod Impact, Unnotched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming. |
|||
Izod Impact, Unnotched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Asia Pacific) 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming. |
|||
Izod Impact, Unnotched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Europe-Africa-Middle East) 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. RoHS compliant. |
|||
Izod Impact, Unnotched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp FX05032 PE (Europe-Africa-Middle East) LNP* THERMOCOMP* FX05032 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added features include : Foaming Agent for Polyolefins.This data was supplied by SABIC-IP for t.. |
|||
Izod Impact, Unnotched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP WX93111 PBT (Europe-Africa-Middle East) LNP* THERMOCOMP* WX93111 is a compound based on Polybutylene Terephalate resin containing Flame retardant , Glass Fiber, Proprietary filler. Added features include : Improved CTI. |
|||
Izod Impact, Unnotched (ISO) | 5.00 kJ/m² @Temperature -20.0 °C |
2.38 ft-lb/in² @Temperature -4.00 °F |
ISO 180/1A |
DSM Arnitel® PL650 Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Izod Impact, Unnotched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starglas FX05032 PE Starglas FX05032 is Polyethylene Resin with a Proprietary Additive (foaming agent for polyolefins)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | |
Axion Polymers Axplas® PS04 0000 Mixed Polystyrene Granules with FR The PS04 series of clean, mixed polystyrene granular chips offers a low-cost option for manufacturers to add post-consumer, engineering polymers to a wide range of products. The polymer mix includes.. |
|||
Izod Impact, Unnotched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO 180/1U |
A.D. Compound Adene NCWA Homopolymer 60% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Izod Impact, Unnotched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | |
Axion Polymers Axplas® PS07 0000 General Purpose Polystyrene PS07 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS07 range of resin co.. |