Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PH 22 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Special designed for automotive light housings. Delivered in natural mo.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -20.0 °C |
14.3 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 69 GF 30 Polypropylene Homopolymer, 30% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -20.0 °C |
14.3 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 69 GF 45 PP, 45% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 45% glass fibre, contains the modifier of mechanical properties.Thermo stable. Increased strength in comparison wit.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -20.0 °C |
14.3 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID® 6 T 30 FRC 4 TS PA6 flame retarded, heat stabilized PA 6 for injection molding, reinforced with 30% mineral filler, flame retarded with nonhalogen flame retardant, heat stabilized. Main features: flammability in accordance with UL 94 3 at 1,6 mm, glo.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVASTER® B1 GF 6/2 PBT reinforced with 6% glass fibre Features: PBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
Qualchem Danamid FGFH-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber. Heat stabilized, for long-lasting use at 120-140°C.Information provided by Qualchem Zrt. |
|||
Charpy Impact Unnotched | 3.01 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Crastin® CE15315 NC010 PBT
(Unverified Data**) Crastin® CE15315 NC010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Rynite® 940 NC010 PET
(Unverified Data**) Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -40.0 °C |
14.3 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® S224-KMV7 Nylon 66-35% Mineral Reinforced (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® Ultraflow™ K-FHGM24 Nylon 6-30% Glass and Mineral Reinforced (European Grade) (Dry)
(discontinued The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® DP 1100/30 H2.0 901510 Nylon 6, Micro Glass Balls PA6, molding grade, micro glass balls, good heat-ageing resistance |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Durethan® DP BM 65 X FM30 901510 Nylon 6, 65% Mineral + Glass Fiber PA, injection molding and hybrid grade based on PA 6, 65% mineral/glass fibers, UL 94V-0 at 1.2 mm, reduced cycle times (easy flow), Thin wall application, free from halogen and phosphorous, low smo.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Pocan® B 7425 000000 PBT, 20% Glass Spheres PBT, 20% glass spheres, injection molding, low tendency to warp, improved surface finish |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® KU 1-7313 000000 PBT + PET, 15% Glass Fiber PBT+PET, 15% glass fibers, injection molding, improved surface finish, increased temperature peak load |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
|
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latamid 66 B G/20-V PA 66, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. High fluidity. Glass fibers. Flame retardant, non classifiable, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific;.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific) Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Noryl V080 PPE+HIPS (Europe-Africa-Middle East) NORYL V080 is an unfilled, flame retardant, high flow material and is halogen free according to VDE/DIN 472 part 815.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® VX8015U PBT+PET (Europe-Africa-Middle East) VALOX VX8015U is a UV stabilized, 15% glass reinforced PBT+PET injection moulding resin with improved surface finish quality characteristics versus VALOX 815. This grade is 815 with improved gloss a.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Asia Pacific) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Arnite® TV4 220 PBT-10% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eU |
DSM EcoPaXX® Q-HXGM24 PA410-(GF+MD)30 % Glass Reinforced, % Mineral Reinforced, Heat Stabilized |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eU |
Eurotec® Tecodur® PB70 KK45 NL XA 20 PBT 45% glass fiber/mineral reinforced, UL94 V0, low warpage Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -20.0 °C |
14.3 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 T 30 Polyamide 6, 30% Micronized Talc FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased tensile modulus - strength of the material. PA matrix reduction. Application for tools, fillin.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |