Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 BT PA6 Basic type PA 6 for compounding, modified for general use. Use: automotive, engineering, electrical and consumer-goods industry. Delivered in the natural mode and in the full RAL color scale.Informa.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 GF 30 002 TS PA6 reinforced with glass fiber, heat stabilized PA 6 for injection molding, reinforced with 30% glass fiber, heat stabilized. Decrease in tensile strength by 50 % after 5000 hours at 170°C. Used for holders of hand tools, hobby tools, gear wheel.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 GF 15 T 6 TS PA66, 15% glass fibre, 6% talc FeaturesChemically reinforced with 15% glass fibre and 6% of talc, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrica.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PP CQX10030 R3 Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PC 99 GF 30/1M Polypropylene reinforced with glass fiber, improved flowing Modified copolymer PP for injection molding, reinforced with 30% glass fiber, improved flowing. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Informatio.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 T 20 PA6, 20% mineral filling FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased modulus in tension - strength of the material. PA matrix reduction. Application eg. for tools, fi.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® Ultraflow™ K-FHGM44 Nylon 6-40% Glass and Mineral Reinforced (European and Asian Grade) (Dry)
(di The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Durethan® DP 1441/40 H2.0 EF 900116 Nylon 6, 40% Glass Fiber + Mineral PA 6, injection molding grade, 40% glass fibers/mineral, good heat-ageing resistance, good surface, good flowability (Easy Flow), low warpage |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® B 4225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, flame retardant |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Pocan® BF 4225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, flame retardant |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® BF 4225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, flame retardant |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latilon 28D G/20 PC, 20% Glass Fiber Reinforced Polycarbonate (PC) based compound. Glass fibers. Low smoke density and low toxicity index. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1fU |
Borealis Nepol™ GB601HP Polypropylene, 20% Long Glass Fiber Reinforced w/BJ356MO Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K222-KGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K222-KWGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eU |
DSM Stanyl® 46SF5030 PA46-GF30 FR(17) 30% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
cond; ISO 179/1eU |
DSM Stanyl® TW241B3 PA46-CF15 15% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eU |
Eurotec® Tecodur® PB70 NL XA 20 PBT unreinforced, UL94 V0 Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eU |
Eurotec® Tecomid® NA40 KK30 NL PA 6.6 30% glass fiber/mineral reinforced, low warpage Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eU |
Eurotec® Tecomid® NA40 GR15 NL PA 6.6 15% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultramid® B3WGM 24 HP BK 23210 10/20% Glass/Mineral Filled PA6-1 (Dry) Description: 20% mineral-filled and 10% glass-fiber reinforced injection-molding grade with outstanding flowability for technical parts with medium rigidity and high dimensional stability, e.g. for.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eU |
Covestro Makroblend® UT4045 G PC/PBT Blend, 20% Glass Filled Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Excellent chemic.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S CV300 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30NHF BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin with improved flow. It is also a PPA resin and it uses a non-halogenated flame ret.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont .. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXALEN PPC343G20 Polypropylene Copolymer, 20% Glass Filled SAXALEN PPC343G20 is a 20% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radiflam® A RV300AE (cond.) Nylon 66-30GF PA66 flame retardant injection molding grade. 30% Glass fiber reinforced, for items with high stiffness. Natural colorInformation provided by Radici group. |