Mechanical Properties Metric English Comments
Charpy Impact Unnotched 18.0 J/cm²

@Temperature 23.0 °C
85.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Lanxess Pocan® B 1305 000000 PBT
PBT, non-reinforced, injection molding
Charpy Impact Unnotched 18.0 J/cm²

@Temperature -30.0 °C
85.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Lanxess Pocan® B 1505 000000 PBT
PBT, non-reinforced, injection molding, extrusion
Charpy Impact Unnotched 18.0 J/cm²

@Temperature 23.0 °C
85.7 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Charpy Impact Unnotched 18.0 J/cm²

@Temperature 23.0 °C
85.7 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Asia Pacific)
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Charpy Impact Unnotched 18.0 J/cm²

@Temperature 23.0 °C
85.7 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Europe-Africa-Middle East)
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Charpy Impact Unnotched 18.0 J/cm²

@Temperature -30.0 °C
85.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Styrolution Luran® S 797 S UV White 33999 Q455 ASA
Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
Charpy Impact Unnotched 18.0 J/cm²

@Temperature -30.0 °C
85.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Styrolution Luran® S 797 S White 35962 ASA
Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
Charpy Impact Unnotched 18.0 J/cm²

@Temperature 23.0 °C
85.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Styrolution Novodur® H604 ABS
Novodur H604 is a high heat injection molding grade with enhanced chemical resistance, especially suitable for being painted.Information provided by Styrolution
Charpy Impact Unnotched 18.0 J/cm²

@Temperature 23.0 °C
85.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Styrolution Novodur® H701 ABS
Novodur H701 is an injection molding grade of ABS with heat resistance and high impact strength.Information provided by Styrolution
Charpy Impact Unnotched 18.0 J/cm²

@Temperature 23.0 °C
85.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1eU
Styrolution Novodur® P2M-AT ABS Pellets
Novodur® P2M-AT has high impact strength, high gloss, and contains antistatic additive. It is used for the production of molded plastic articles.
Charpy Impact Unnotched 18.0 J/cm²

@Temperature 23.0 °C
85.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1eU
Styrolution Novodur® P2M-V ABS Pellets
Novodur® P2M-V has high impact strength, high gloss, and low emission. It is used for the production of molded plastic articles.
Charpy Impact Unnotched 18.0 J/cm²

@Temperature 23.0 °C
85.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Styrolution Terlux® 2802 TR Q434 Transparent MABS
Description: Terlux® 2802 TR Q434 is a new grade with enhanced toughness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Charpy Impact Unnotched 18.0 J/cm²

@Temperature -30.0 °C
85.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Styrolution Novodur® 5300 ABS
Novodur 5300 is a high heat injection molding grade with high impact strength, good chemical resistance and reduced emission (PC modified)Information provided by Styrolution
Charpy Impact Unnotched 18.0 J/cm²

@Temperature 23.0 °C
85.7 ft-lb/in²

@Temperature 73.4 °F
DIN ISO 179
BASF Elastollan R 2001 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Charpy Impact Unnotched 18.0 J/cm²

@Temperature 23.0 °C
85.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultraform® S2320 003 POM
Description: Easy flowing and rapidly freezing grade for injection molding difficult, thin-walled part.Information provided by BASF
Charpy Impact Unnotched 18.0 J/cm²

@Temperature 23.0 °C
85.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultraform® S2320 003 PRO BK 00120 POM
Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF
Charpy Impact Unnotched 18.0 J/cm²

@Temperature 23.0 °C
85.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultraform® S2320 003 PRO POM
Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF
Charpy Impact Unnotched 18.0 J/cm²

@Temperature -30.0 °C
85.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® W2320 0035 POM
Description: Is a POM, very free-flowing and rapidly solidifying grade for high processing demands.Information provided by BASF
Charpy Impact Unnotched 18.0 J/cm²

@Temperature 23.0 °C
85.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultraform® W2320 0035 POM
Description: Is a POM, very free-flowing and rapidly solidifying grade for high processing demands.Information provided by BASF
Charpy Impact Unnotched 18.0 J/cm²

@Temperature 23.0 °C
85.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultraform® W2320 0035 LEV POM
Description: Is a POM, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF
Charpy Impact Unnotched 18.0 J/cm²

@Temperature -30.0 °C
85.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® W2320 0035 LEV POM
Description: Is a POM, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF