Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 4.50 MPa | 653 psi | ISO 37 |
PolyOne OnFlex™ S FR 40A-3S1841 Thermoplastic Elastomer (TPE) OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo.. |
|||
Tensile Strength at Break | 4.50 MPa | 653 psi | ISO 37 |
PolyOne OnFlex™ S KA 60A-3S1769 Thermoplastic Elastomer (TPE) OnFlex™-S KA thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tensile Strength at Break | <= 4.50 MPa | <= 653 psi | ISO/R527 |
Polykemi AB POLYelast TPE Z406 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Tensile Strength at Break | 4.50 - 6.00 MPa | 653 - 870 psi | DIN 53504 S2 |
Wacker Silicones Geniomer® 140 Silicone TPE SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |
|||
Tensile Strength at Break | 4.50 MPa | 653 psi | ISO 527 |
A. Schulman INVISION™ VX-5065UI Soft Touch Polyolefin Thermoplastic ApplicationInvision™ VX-5065UI is targeted for automotive injection molding appearance applications. Information provided by A. Schulman. |
|||
Tensile Strength at Break | 4.50 MPa | 653 psi | ISO 527 |
A. Schulman INVISION™ VX-5065UI Soft Touch Polyolefin Thermoplastic ApplicationInvision™ VX-5065UI is targeted for automotive injection molding appearance applications. Information provided by A. Schulman. |
|||
Tensile Strength at Break | 4.50 MPa | 653 psi | ISO 527 |
A. Schulman INVISION™ VX-5065UI Soft Touch Polyolefin Thermoplastic ApplicationInvision™ VX-5065UI is targeted for automotive injection molding appearance applications. Information provided by A. Schulman. |
|||
Tensile Strength at Break | 4.50 MPa | 653 psi | ISO 527 |
A. Schulman INVISION™ VX-5065UI Soft Touch Polyolefin Thermoplastic ApplicationInvision™ VX-5065UI is targeted for automotive injection molding appearance applications. Information provided by A. Schulman. |
|||
Tensile Strength at Break | 4.50 MPa | 653 psi | ISO 527 |
A. Schulman INVISION™ VX-5065UI Soft Touch Polyolefin Thermoplastic ApplicationInvision™ VX-5065UI is targeted for automotive injection molding appearance applications. Information provided by A. Schulman. |
|||
Tensile Strength at Break | 4.50 MPa | 653 psi | Air at 302°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 121-58W175 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for .. |
|||
Tensile Strength at Break | 4.50 MPa | 653 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Tensile Strength at Break | 4.50 MPa | 653 psi | ASTM D638 |
Arkema Group OREVAC® 9305 EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Tensile Strength at Break | 4.50 MPa | 653 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX E 55.1 TPE-V, Shore A55 TPE-VInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength at Break | 4.50 MPa | 653 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX S 45 A.01 TPE-S, Shore A45, translucent TPE-SInformation provided by BARLOG plastics GmbH. |