Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group OREVAC® 9305 EVA Terpolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Arkema
Trade Name OREVAC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group OREVAC® 9305 EVA Terpolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as free flowing natural coloured granules. Applications include thermo-adhesive films and hot melt adhesives.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ASTM D1505
Vinyl Acetate Content 26 - 30 %
26 - 30 %
Arkema
Melt Index of Compound 150 - 210 g/10 min

@Load 2.16 kg,
Temperature 190 °C
150 - 210 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 71
71
ASTM D2240
Tensile Strength at Break 4.50 MPa
653 psi
ASTM D638
Tensile Strength, Yield 1.80 MPa
261 psi
ASTM D638
Elongation at Break 700 - 900 %
700 - 900 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 68.0 °C
154 °F
DSC
Vicat Softening Point <= 40.0 °C
<= 104 °F
ASTM D1525
Ring & Ball Softening Point 92.0 °C
198 °F
Descriptive Properties Value Comments
MAH Mini 6400