Barlog Plastics KEBAFLEX S 45 A.01 TPE-S, Shore A45, translucent

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Barlog Plastics
Trade Name KEBAFLEX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBAFLEX S 45 A.01 TPE-S, Shore A45, translucent.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TPE-SInformation provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.043 cm/cm
0.043 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cm
0.012 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
Tensile Strength at Break 4.50 MPa
653 psi
ISO 527-1
Elongation at Break 450 %
450 %
ISO 527-1
Descriptive Properties Value Comments
Resin Type TPE-S