Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 16.5 MPa | 2400 psi | 2 in/min; ASTM D638 |
RheTech Products FT2500-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | 2 in/min; ASTM D638 |
RheTech Products FT2500-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | 2 in/min; ASTM D638 |
RheTech Products FT2500-594UV Thermoplastic Polyolefin, UV Stabilized, 9428NM Spectra Grey Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | 2 in/min; ASTM D638 |
RheTech Products FT3150-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air deflectorsUnderhood componentsBumper componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | 2 in/min; ASTM D638 |
RheTech Products FT7012-707UV Thermoplastic Polyolefin, UV Stabilized, 848 Black Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | TM R050-36 |
Resinlab® EP1294 Mineral Filled, Flame Retardant Epoxy Syntactic Foam Resinlab™ EP1294 is a two part mineral filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-exti.. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | ASTM D638 |
LyondellBasell Petrothene® PR92735 Linear Low Density Polyethylene ApplicationsPETROTHENE PR 92735 is a high molecular weight, linear low density-based compound designed for cable jacketing. PR 92735 contains a nominal carbon black content of 2.6% and antioxidant .. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | 100% retained after aging 7 days at 165°C.; ASTM D638 |
LyondellBasell Petrothene® YR19548 Polyolefin Compound ApplicationsPETROTHENE YR 19548 is a colorable, thermoplastic non-halogenated, flame retardant polyolefin compound formulated for small gauge automotive primary insulation (SAE J1128) and appliance .. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | ASTM D412 |
ITW Devcon Flexane® Rubber Repair / Castable Urethane Fast Cure, Black Information provided by ITW Devcon |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | ASTM D412 |
Teknor Apex APEX® 2075-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-ClearForms-PelletsProcessing Method-Extrusi.. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | ASTM D638 |
Teknor Apex APEX® 3600-75NT Polyvinyl Chloride, Flexible Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: First Generation SeriesInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | ASTM D638 |
Teknor Apex APEX® 4124 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Features: Good UV Resistance; Sunlight Resistant (720 hours) Uses: Appliance Wire Jacketing; Irrigation Cable Jacketing Forms: Pellets Wire Types: UL Style 2464.. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | ASTM D638 |
Teknor Apex APEX® 460 Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Features: Low to no Migration; Oil Resistant Uses: Flexible Cord InsulationForms: Pellets Wire Types: SJTOO; STOO Processing Method: Extrusion Additional I.. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | ASTM D412 |
Teknor Apex MF 573 Polyvinyl Chloride, Flexible Film Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsInformation provided by Teknor Apex Company |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | ASTM D638 |
Teknor Apex APEX® 80842 Polyvinyl Chloride, Flexible Notes: 105°C Jacket; RoHS Compliant Features: High Heat Resistance; Sunlight Resistant (720 hours) Uses: Outdoor Applications; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL Qmtt2.. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | ASTM D412 |
Teknor Apex Telcar® TL EF-6133L2 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | ASTM D412 |
Teknor Apex Telcar® TL-1017A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | ASTM D412 |
Teknor Apex Telcar® TL-1154A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | ASTM D412 |
Teknor Apex Telcar® TL-1155B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | ASTM D412 |
Teknor Apex Telcar® TL-2478K Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | ASTM D412 |
Teknor Apex Telcar® TL-8451 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | ASTM D412 |
Teknor Apex Telcar® TL-88-N809K Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | ASTM D412 |
Teknor Apex Uniprene® UN-2467A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow FLEXOMER™ GRSN-1539 NT 7 Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ GRSN-1539 NT 7 is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins .. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | ASTM D638 |
Chesterton ARC MX5 Rapid Curing Fine Particle Wear Compound Description: An advanced ceramic reinforced composite for the emergency repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a th.. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FE 5643Q Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FE 5643Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu.. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FE 5660Q Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FE 5660Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu.. |
|||
Tensile Strength at Break | 16.5 MPa | 2400 psi | ASTM D638 |
Bayshore Vinyl Compounds BVC 1100-78 Clear PVC Compound BVC 1100-78 is a clear flexible PVC compound produced with FDA sanctioned ingredients. It is recommended for use in applications for the medical, food and beverage industries. This material offers.. |