3M Dyneon™ FE 5643Q Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer 3M Dyneon™
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ FE 5643Q Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Dyneon™ Fluoroelastomer FE 5643Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The “dry” ingredients should be blended before adding to the masticated gum. For best results, FE 5643Q should be banded on the mill several minutes prior to adding the blended dry ingredients. Once mixed, the compounded stocks have good scorch resistance and storage stability.Composition: Di-polymer of vinylidene fluoride and hexafluoropropyleneFaster curing version of FE 5640QProcess target: compression moldingImproved scorch resistance over Dyneon 2000 series at high molding temperaturesProprietary incorporated cure technologyExcellent mold releaseImproved cure technology over Dyneon 2000 series resulting in more consistent part size from successive molding cyclesClean runningInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
Mooney Viscosity 40

@Temperature 121 °C
40

@Temperature 250 °F
ML1+10
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C; ASTM D2240
Tensile Strength at Break 16.5 MPa
2400 psi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Elongation at Break 180 %
180 %
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
100% Modulus 0.00772 GPa
1.12 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Compression Set 11 %
11 %
Aged 70 hours @ 200°C, -214 O-rings; ASTM D395 Method B
Thermal Properties Metric English Comments
Transformation Temperature -18.0 °C
-0.400 °F
TR10; ASTM D1329
Component Elements Properties Metric English Comments
Fluorine, F 65.9 %
65.9 %
Descriptive Properties Value Comments
Color Opaque Off-White
MH, Maximum Torque 22 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
24.9 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
ML, Minimum Torque 1.3 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
1.6 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
Solubility Ketones and Esters
t`50, Time to 50% cure 0.5 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
1.5 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
t`90 - Time to 90% cure 0.6 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
2.1 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
ts2 - Time to 2 in-lb rise from min 0.4 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
1.2 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289