Polymer Property : Tensile Strength at Break = 81.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 81.4 MPa
11800 psi
ASTM D638
PolyOne Stat-Tech™ ST9620-0020 ES Red Liquid Crystal Polymer + PPS (LCP+PPS)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Tensile Strength at Break 81.4 MPa
11800 psi
ASTM D638
Ravago Manufacturing Americas Hylon® N1020MHL Nylon 6/6  (discontinued **)
Available in North America Filler: Mineral, 20% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedForm: Pellets Processing Method: Injection MoldingIn..
Tensile Strength at Break 81.4 MPa
11800 psi
ASTM D638
Firestone CLM200-001 Nylon 6
Used for monofiliament extrusion. Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone
Tensile Strength at Break 81.4 MPa

@Thickness 3.20 mm
11800 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical Lupox® TE5100 PBT+PC+GF10%
Description: Injection Molding, PBT+PC+GF10%, High Impact resistant, Dimensional StabilityApplication: Automotive (Bumper Back Beam)CAS No. 30965-26-5, 103598-77-2 and 65997-17-3Information provided..
Tensile Strength at Break 81.4 MPa
11800 psi
ASTM D638
Plastics Group Polifil® 628L Nylon 6/6 (DAM)
Polifil® NYLON 6/6 combines good abrasion and chemical resistance.Applications: ValvesBearingsBearing casesStandard processing techniques are applicable. Information provided by The Plastics Group...
Tensile Strength at Break 81.4 MPa
11800 psi
ASTM D638
Chase Plastics CP Pryme® N333GL (COND, 50% RH) Nylon 6 (Utility Grade), 33% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
Tensile Strength at Break 81.4 MPa
11800 psi
ASTM D638
Plastics Group Polifil® GFPPCC-20 20% Glass Reinforced Polypropylene
Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature..