Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.21 MPa | 900 psi | ASTM D638 |
Reltek BONDiT™ HM-502 Coating, Sealant, Adhesive System A protective coat for most metal, glass, and ceramic materials for use against corrosion and other chemical attacks. Useful against fungi growth. Bondit HM-502 is a thermoplastic emulsion system.Inf.. |
|||
Tensile Strength at Break | 6.21 MPa | 900 psi | ASTM D638 |
Reltek BONDiT™ HM-505 Coating, Sealant, Adhesive System Information provided by Reltek LLC |
|||
Tensile Strength at Break | 6.21 MPa | 900 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 111-64 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Tensile Strength at Break | 6.21 MPa | 900 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8291-85PA Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/s.. |
|||
Tensile Strength at Break | 6.21 MPa | 900 psi | ASTM D412 |
Multibase Multi-Flex® A 6221 E Black TPE Thermoplastic Elastomer Forms: PelletsInformation provided by Multibase |
|||
Tensile Strength at Break | 6.21 MPa | 900 psi | ASTM D412 |
Teknor Apex Monprene® MP 1085 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 6.21 MPa | 900 psi | ASTM D412 |
Teknor Apex Monprene® MP 2104 Thermoplastic Elastomer Features: Nice Silken Feel Uses: Safety ProductsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 6.21 MPa | 900 psi | ASTM D412 |
Teknor Apex Monprene® MP-2123 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 6.21 MPa | 900 psi | ASTM D412 |
Teknor Apex Monprene® MP-2830C CLR Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 6.21 MPa | 900 psi | ASTM D412 |
Teknor Apex Telcar® OBC 4773A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 6.21 MPa | 900 psi | ASTM D412 |
Teknor Apex Telcar® TL-1654G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 6.21 MPa | 900 psi | ASTM D412 |
Teknor Apex Telcar® TL-2519E Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Tensile Strength at Break | 6.21 MPa | 900 psi | ASTM D412 |
Teknor Apex Telcar® TL-2597 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 6.21 MPa | 900 psi | ASTM D412 |
Teknor Apex Telcar® TELC 1025-70 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 6.21 MPa | 900 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow 959S Linear Low Density Polyethylene (LDPE) DOW Polyethylene 959S is a medium molecular weight distribution homopolymer. This resin has good process-ability over a wide range of molding conditions. Typical applications include lids. It com.. |
|||
Tensile Strength at Break | 6.21 MPa | 901 psi | |
3M Scotchkote™ 60RG 537 Urethane Elastomer Scotchkote Urethane Elastomer 60RG 537 has been specifically developed as a fast curing elastomeric repair system with a high degree of flexibility for rebuilding and resurfacing rubber components.P.. |
|||
Tensile Strength at Break | 6.21 MPa | 900 psi | ASTM D412 |
Aaron Industries AAROPRENE® ATPR ECATPR2040 Black Thermoplastic SEBS Rubber AAROPRENE® ATPR 2000 Series Elastomeric CompoundFeatures: A black, thermoplastic SEBS Rubber compound specifically designed for the injection molding of industrial gaskets. |
|||
Tensile Strength at Break | 6.21 MPa | 900 psi | ASTM D412 |
Teknor Apex Monprene® MP-2691A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |