Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 27.6 MPa | 4000 psi | 2 in/min; ASTM D638 |
RheTech Products T40P100-774UVA 40% Talc Reinforced Polypropylene, UV Stabilized, JA6A Black Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxDoor cup pullsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | TM R050-36 |
Resinlab® EP965LVLX Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965LVLX Black is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has .. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D 638 type IV |
Total Finathene® 3802N Natural HDPE pipe grade
(discontinued **) Applications: Natural gas distribution, extruded pipes, molded fittings, pipe coating, pipe liningInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and .. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D4894 |
3M Dyneon™ 1641 PTFE Powder
(discontinued **) Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D4894 |
3M Dyneon™ TR 1105 PTFE
(discontinued **) Ideal for thin wall ram extrusion productsReduces cold flow and melt viscosityLower permeabilityLower porosityWeldableExcellent product smoothnessIncreased machine outputInformation provided by Dyne.. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
LyondellBasell Petrothene® HR92953 Medium Density Polyethylene ApplicationsPETROTHENE HR 92953 is a medium density polyethylene-based resin designed for use as jacketing for communications cable, including CATV and FOC. HR 92953 has a nominal carbon black cont.. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
ITW Devcon Metal Repair Titanium Putty, Grey Information provided by ITW Devcon |
|||
Tensile Strength at Break | 27.6 - 31.0 MPa | 4000 - 4500 psi | |
ITW Plexus Plexusâ„¢ MA310 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Use with "difficult to bond" plastics, high strength.Information provided by Illinois Tool Works. |
|||
Tensile Strength at Break | 27.6 - 31.0 MPa | 4000 - 4500 psi | |
ITW Plexus Plexusâ„¢ MA350 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low viscosity adhesive, high strength, especially suitable for battery case applications.Informati.. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | 2.0 in/min; ASTM D412 |
Teknor Apex Telcar® TL-1377A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | >= 27.6 MPa | >= 4000 psi | |
Master Bond EP37-3FLFAN Electrically Isolating, Flexible Epoxy Description: Master Bond Polymer System EP37-3FLFAN is a two component system for high performance potting, bonding, sealing and coating that is formulated to cure at room temperature or more rapidl.. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
Total 5502 HDPE, blow molding, pipe Drug Master File listed; USP Class VI approved; FDA compliant; UL 94HB/746 certified |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
A. Schulman COMTUF® 420 Impact Modified PBT Information provided by A. Schulman. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
Chesterton ARC 10 Paste grade machinable composite Description: A reinforced composite for the repair and protection of metal surfaces. It is machinable with excellent compressive strength, chemical resistance and corrosion resistance. It is non-sag.. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
Eastman Tenite 285A2R30020 Cellulose Acetate Butyrate, Natural, Trsp Applications:Tool handlesToys/sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clar.. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
Entec Hypel® PEHD18/.956 HDPE Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 Die C |
3M Scotch-Weld™ TE200 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
Americas Styrenics STYRON® 487 High Impact Polystyrene Product CharacteristicsGood TrimmabilityToughnessHeat resistanceFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliancesPackaging/disposablesHousewaresInformation provided by A.. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | TM R050-36 |
Resinlab® EP965LVLX Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965LVLX Clear is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has .. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | TM R050-36 |
Resinlab® EP1190 Flame Retardant Epoxy Casting Resin Resinlab™ EP1190 is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Proje.. |