Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 235 MPa | 34100 psi | |
Plastcom SLOVAMID 6 GF 65 PA6, 65% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Tensile Strength at Break | 235 MPa | 34100 psi | ASTM D638 |
Niche Polymer PA66GF50BK Nylon 66, 50% Glass Fiber Filled Information provided by Niche Polymer |
|||
Tensile Strength at Break | 235 MPa @Temperature 23.0 °C |
34100 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® HTN 52G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provide.. |
|||
Tensile Strength at Break | 235 MPa | 34100 psi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA)
(Unverified Data**) Ixef 1622 is an impact modified, 50% glass-fiber reinforced polyarylamide. which exhibits very high strength and rigidity, outstanding surface gloss, and excellent impact resistance. - Natural: Ixef.. |
|||
Tensile Strength at Break | 235 MPa | 34100 psi | ISO 527-1/-2 |
DSM Akulon® K-FHG12 (Dry) 60% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Strength at Break | 235 MPa | 34100 psi | ISO 527-1/-2 |
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Strength at Break | 235 MPa | 34100 psi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: Good.. |
|||
Tensile Strength at Break | 235 MPa | 34100 psi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1622 is an impact modified, 50% glass-fiber reinforced polyarylamide. which exhibits very high strength and rigidity, outstanding surface gloss, and excellent impact resistance.Features: Go.. |
|||
Tensile Strength at Break | 235 MPa | 34100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP PF00DS PA 6 (Europe-Africa-Middle East) LNP THERMOCOMP* PF00DS is a compound based on PA6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Strength at Break | 235 MPa | 34100 psi | ISO 527-93 |
Wellman Wellamid® GF1750-N2 50% Glass Fiber Reinforced Nylon 6 Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman. |
|||
Tensile Strength at Break | 235 MPa | 34100 psi | ISO 527-1/-2 |
DSM Akulon® Ultraflow™ K-FHG12 Nylon 6-60% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Strength at Break | 235 MPa | 34100 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GVL-5H nat PA*-GF50 Product description: Grivory GVL-5H natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H na.. |
|||
Tensile Strength at Break | 235 MPa | 34100 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HTV-45H1 black 9205 PA6T/6I-GF45 Product description: Grivory HTV-45H1 black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation a.. |
|||
Tensile Strength at Break | 235 MPa | 34100 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 52G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced PPA High Performance Polyamide Zytel HTN52G45HSL BK083 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin that can be molded in water heated m.. |
|||
Tensile Strength at Break | 235 MPa | 34100 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN LT51G35HSLR BL661A Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Laser Weldable PPA High Performance Polyamide Information provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 235 MPa | 34100 psi | ISO 527 |
Eurotec® Tecomid® NA40 GR50 NL PA 6.6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Strength at Break | 235 MPa | 34100 psi | ISO 527 |
Eurotec® Tecomid® NAX0 GR60 NL PA6.6, 60% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Tensile Strength at Break | 235 MPa @Temperature 23.0 °C |
34100 psi @Temperature 73.4 °F |
ISO 527-2 |
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA)
(Unverified Data**) Ixef 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 102.. |