Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 230 MPa | 33400 psi | STN EN ISO 527-2 |
Plastcom SLOVAMID 66 GF 50 Polyamide 66, 50% Glass Fiber FeaturesChemically reinforced with 50% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | ISO 527-1/-2 |
DSM Akulon® K-FHG0 (Dry) 50% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | ISO 527 |
Solvay Technyl® A218V43 43% Glass Filled, Heat Stabilized Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance.Features: Flame Ret.. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | ISO 527 |
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66 Information provided by A. Schulman. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | ISO 527 |
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66 Information provided by A. Schulman. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | ASTM D638 |
Unitika E-RUNG60 Ultra high-rigidity PA6, Conditioned Ultra high-rigidityInformation provided by Unitika Ltd. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | ISO 527 |
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66 Information provided by A. Schulman. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | ISO 527 |
A. Schulman SCHULAMID® 66 GF50H 50% Glass Fiber Reinforced, Heat Stabilized 66 Information provided by A. Schulman. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | ISO 527 |
A. Schulman SCHULAMID® 66 GF50H 50% Glass Fiber Reinforced, Heat Stabilized 66 Information provided by A. Schulman. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | ISO 527 |
A. Schulman SCHULAMID® 66 GF50H 50% Glass Fiber Reinforced, Heat Stabilized 66 Information provided by A. Schulman. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-40 S PA6-GF40 Product description: Grilon BG-40 S is a normal viscosity PA 6 injection molding type with 40% glass fibers. Grilon BG-40 S has the following important properties: High stiffnessExcellent surface fi.. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-4 FWA black 9225 PA*-GF40 Product description: Grivory GV-4 FWA black 9225 is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-4 FWA nat PA*-GF40 Product description: Grivory GV-4 FWA natural is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam.. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | ISO 527-1/-2 |
DSM Stanyl® TW241F8 Nylon 46-40% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4065 black 9238 PA*-GF50 Product description: Grivory XE 4065 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL BK083 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | ISO 527-1/-2 |
DSM Akulon® Ultraflow™ K-FHG0 Nylon 6-50% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVL-4H black 9915 PA*-GF40 Product description: Grivory GV-6H EF natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | ISO 527 |
Eurotec® Tecomid® NA40 KC50 BK111 PA6.6, 50% glass/carbon fiber reinforced, black Information provided by Eurotec® |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | 5 [mm/min]; ISO 527-1/2 |
Akro-Plastic Akroloy® PA GF 40 (2845) PA 6.6 & PA6I/6T Dry, 40% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Tensile Strength at Break | 230 MPa @Temperature -40.0 °C |
33400 psi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Dry) Ultramid 8233G HS BK-102 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature performance and d.. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-4H black PA*-GF40 Product description: Grivory GV-4H black 9915 is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | ISO 527 |
A. Schulman SCHULAMID® 66 GF50H 50% Glass Fiber Reinforced, Heat Stabilized 66 Information provided by A. Schulman. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Verton PV00A PA 6 LNP VERTON* PV00A is a compound based on Nylon 6 resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | ISO 527 |
SABIC Innovative Plastics LNP Verton UX06451 BK8-312 PPA LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength at Break | 230 MPa | 33400 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 73G45L NC010 Nylon 6
(Unverified Data**) 45% Glass Reinforced Polyamide 6Zytel 73G45L NC010 is a 45% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 230 MPa @Temperature 23.0 °C |
33400 psi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |