Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.70 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
6.93 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne Gravi-Tech™ GT6000-0023 Black Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Izod Impact, Unnotched | 3.70 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
6.93 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D4812 |
PolyOne Geon™ 83510 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Unnotched | 3.70 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
6.93 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne Gravi-Tech™ GRV-NP-110-W-NAT Polyamide 12 (Nylon 12) Information provided by PolyOne |
|||
Izod Impact, Unnotched | 3.70 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
6.93 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® 12-031
(discontinued **) PRE-ELEC 12-031 is a conductive thermoplastic compound based on a polyacetal copolymer with 10% carbon fiber. PRE-ELEC 12-031 exhibits excellent mechanical properties and electrical conductivity. Te.. |
|||
Izod Impact, Unnotched | 3.70 J/cm | 6.93 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI) Torlon® 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon® PAI grades cannot be molded successfully in molds with undercuts. Torlon® 4601 has been formulated to.. |
|||
Izod Impact, Unnotched | 3.70 J/cm | 6.93 ft-lb/in | ASTM D256 |
Covestro Baydur® GS-772 Polyurethane Solid RIM, MDI-based 2-Component Liquid System 0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Izod Impact, Unnotched | 3.70 J/cm @Temperature -40.0 °C |
6.93 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Adell ER-19 Polypropylene Homopolymer; 43% Glass Reinforced, High Stiffness Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 3.70 J/cm @Temperature -40.0 °C |
6.93 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Adell ER-39 Polypropylene Homopolymer; 43% Glass Reinforced, High Stiffness Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 3.70 J/cm | 6.93 ft-lb/in | ASTM D256 |
Adell RA-16 Copolymer Polypropylene, 30% Talc Filled Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 3.70 J/cm | 6.93 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 5002 Polyarylamide (PARA), 20% GlassPTFE
(discontinued **) Ixef 5002 is a 20% glass-fiber reinforced, PTFE modified polyarylamide which exhibits very good mechanical performance, very good surface gloss, and superior wear properties.- Natural: Ixef 5002/008.. |
|||
Izod Impact, Unnotched | 3.70 - 3.70 J/cm @Temperature -40.0 - -40.0 °C |
6.93 - 6.93 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 3.70 J/cm Grade Count:2 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |