Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Baydur® GS-772 Polyurethane Solid RIM, MDI-based 2-Component Liquid System

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Solid RIM
Manufacturer Covestro
Trade Name Baydur®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Baydur® GS-772 Polyurethane Solid RIM, MDI-based 2-Component Liquid System.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
Bayer Test
Mechanical Properties Metric English Comments
Hardness, Shore D 76
76
ASTM D2240
Tensile Strength, Ultimate 39.0 MPa
5660 psi
ASTM D638/D412
Elongation at Break 10 %
10 %
ASTM D638/D412
Flexural Yield Strength 60.0 MPa
8700 psi
ASTM D790
Flexural Modulus 1.40 GPa
203 ksi
ASTM D790
Compressive Yield Strength 35.0 MPa
5080 psi
ASTM D395
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.70 J/cm
6.93 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 101 µm/m-°C

@Temperature 20.0 °C
56.1 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C
210 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 6.35 mm
V-0

@Thickness 0.250 in
V-0

@Thickness 6.35 mm
V-0

@Thickness 0.250 in
Electrical Properties Metric English Comments
Electrical Resistivity 2.30e+14 ohm-cm
2.30e+14 ohm-cm
ASTM D257
Surface Resistance 3.10e+15 ohm
3.10e+15 ohm
ASTM D257
Dielectric Constant 3.44

@Frequency 1e+6 Hz
3.44

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 11.5 kV/mm
292 kV/in
ASTM D149