Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 9.40 J/cm @Thickness 3.17 mm |
17.6 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Performance Polymers IPS II PPL-C4270 PEKK (Polyetherketoneketone) Linear 40% Carbon Fiber Reinforced Molding Grade Black pelletsInformation provided by Infinite Polymer System II. |
|||
Izod Impact, Unnotched | 9.39 J/cm | 17.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RFL46ES PA 66 LNP* LUBRICOMP* RFL46ES is a compound based on Nylon 6/6 containing 30% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Heat Stabilized, Easy Molding. |
|||
Izod Impact, Unnotched | 9.39 J/cm | 17.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP UCL36S PPA LNP* LUBRICOMP* UCL36S is a compound based on Polyphthalamide resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Heat Stabilized, Electrically Con.. |
|||
Izod Impact, Unnotched | 9.39 J/cm | 17.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP UCL36S PPA (Asia Pacific) LNP* Lubricomp* UCL36S is a compound based on Polyphthalamide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Heat Stabilized, Electrically Cond.. |
|||
Izod Impact, Unnotched | 9.40 J/cm | 17.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DX11408 PC LNP* STAT-KON* DX11408 is a compound based on Polycarbonate containing Carbon Powder. Added features of this material include: Electrically Conductive, Improved Ductility |
|||
Izod Impact, Unnotched | 9.39 J/cm | 17.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF00AH PA 66 LNP* THERMOCOMP* RF00AH is a compound based on Nylon 66 resin containing 50% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Izod Impact, Unnotched | 9.39 J/cm | 17.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF00AH PA 66 (Asia Pacific) LNP* Thermocomp* RF00AH is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Izod Impact, Unnotched | 9.39 J/cm | 17.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA 6/10 LNP LUBRICOMP* QFL36 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Unnotched | 9.39 J/cm @Thickness 3.18 mm |
17.6 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Lubricomp® QFL-4036 BK8-115 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
(disconti Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Izod Impact, Unnotched | 9.38 J/cm @Temperature 23.0 °C |
17.6 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Verton RV006ESV_GY7E071 PA 66 Preliminary Data for 30% long glass fiber, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region. |