Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.83 J/cm | 12.8 ft-lb/in | ASTM D256 |
LNP ULTEM® SMU6303 Polyetherimide, 5% Glass Fiber Reinforcement, 5% PTFE Lubricant
(discontinued **) Will be UNTW05.Features: Lubricated, High Heat Resistance, Good Wear Resistance, Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provide.. |
|||
Izod Impact, Unnotched | 6.85 J/cm | 12.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RFG16S PA 66 LNP* LUBRICOMP* RFG16S is a compound based on Nylon 66 resin containing 5% Graphite, 30% Glass Fiber. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Unnotched | 6.83 J/cm | 12.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RL4040HSUV PA 66 LNP* LUBRICOMP* RL4040HSUV is a compound based on Nylon 66 containing 20% PTFE. Added features of this grade include: Heat Stabilized, UV Stabilized, Wear Resistant. |
|||
Izod Impact, Unnotched | 6.83 J/cm | 12.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 LNP* LUBRICOMP* SP003 is a compound based on Nylon 12 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched | 6.83 J/cm | 12.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 (Asia Pacific) LNP* Lubricomp* SP003 is a compound based on Nylon 12 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 6.83 J/cm | 12.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP WFL34 PBT LNP LUBRICOMP* WFL34 is a compound based on PBT resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Unnotched | 6.83 J/cm | 12.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT LNP LUBRICOMP* WFL36 is a compound based on PBT resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Unnotched | 6.83 J/cm | 12.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Asia Pacific) LNP LUBRICOMP* WFL36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 6.84 J/cm | 12.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DEF42 PC LNP STAT-KON* DEF42 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 6.83 J/cm | 12.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA LNP* THERMOCOMP* UF006H is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Izod Impact, Unnotched | 6.83 J/cm | 12.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA (Asia Pacific) LNP* Thermocomp* UF006H is a compound based on Polyphthalamide resin containing Glass Fiber. |
|||
Izod Impact, Unnotched | 6.81 J/cm | 12.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP WX88406 Polyester, TP LNP* Thermocomp* WX88406 is a compound based on Polyester, TP resin. |